Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 245 - 280 °C | 473 - 536 °F | Do not melt above 310°C |
Nilit Nilamid B3 H G8 40% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G8 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key character.. |
|||
Melt Temperature | 245 - 280 °C | 473 - 536 °F | Do not melt above 310°C |
Nilit Nilamid B3 H G3 15% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 6. These products combine good overall mechanical performance and impact strength with ease of processing. Key cha.. |
|||
Melt Temperature | 245 - 270 °C | 473 - 518 °F | Start Point: 260°C |
Kingfa LONOY 3010 Glass Fiber Reinforced PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingElectric and electronic partsBusiness machine cabinetGarden to.. |
|||
Melt Temperature | 245 - 265 °C | 473 - 509 °F | Start Point: 255°C |
Kingfa PA66-ROW Halogen-free, Flame Retardant PA66 Features:Flame retardantHigh mechanical strengthHigh heat resistanceGood electric propertiesNo bloomingApplications:Injection moldingConnectors, linkersRelay, bobbins, plugsHousehold appliance parts.. |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical LUMAX HR5107 PBT+ABS+GF10%, Heat Resistance Description: Injection Molding Grade, PBT+ABS+GF10%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5, 25038-59-9 and 9003-54-7Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2156FL PBT+GF15% Description: Injection Molding, PBT+GF15%, Flame Retardant Application: IT/OA, E&E (CRT Socket)CAS No. 68928-70-1, 71342-77-3, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by.. |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2306FB PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2306FC PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2306FI PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant, High Impact Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical.. |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® LW5402A PBT+PC+GF40% Description: Injection Molding, PBT+PC+GF40%, Low Warpage, High GlossApplication: E&E, Automotive (Bobbin, Switch)CAS No. 9010-86-0, 65997-17-3, 24968-12-5 and 103598-77-2Information provided by LG .. |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® SG3180S PBT+PET+MF18% Description: Injection Molding, PBT+PET+MF18%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Melt Temperature | 245 - 275 °C | 473 - 527 °F | Injection Molding |
LG Chemical LUPOY ER5151RFA PC/ABS Mineral Filler, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High strength, EPEATApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9, 181028-79-5 and 14807-96-6Information p.. |
|||
Melt Temperature | 245 - 285 °C | 473 - 545 °F | Injection Molding |
LG Chemical LUPOY GN1008RF PC, Halogen Free, Flame Retardant, High impact strength Description: Injection Molding, PC, Halogen Free Flame Retardant, High impact strengthApplication: IT&OA (Notebook PC battery pack housing)CAS: 103598-77-2, 137050-02-03 and 139189-30-3Information p.. |
|||
Melt Temperature | 245 - 275 °C | 473 - 527 °F | Injection Molding |
LG Chemical LUPOY SG5009F PC/ABS Description: Injection Molding, PC/ABS, High Gloss, Scratch Resistance, Halogen Free Flame RetardantApplication: IT&OA (Notebook PC & Monitor housing)CAS: 103598-77-2 and 181028-79-5Information prov.. |
|||
Melt Temperature | 245 °C | 473 °F | LCL-PR29 |
Intercontinental Polymers 188 PET Polymer Type - Clear, Alkali Soluble, Polyester Pellets Applications: Filament SpecialtiesInformation provided by Intercontinental Polymers. |
|||
Melt Temperature | 245 - 260 °C | 473 - 500 °F | ISO 294 |
Gromax BTE45-DN00N1 Nylon 6 (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 245 - 260 °C | 473 - 500 °F | ISO 294 |
Gromax BTE45-DN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 245 - 275 °C | 473 - 527 °F | Injection Molding |
LG Chemical LUPOY GN5001RFD PC/ABS, High Impact Description: Injection Molding, PC/ABS, General Purpose, High Impact, Halogen Free Flame retardantApplication: IT&OA (Notebook PC housingCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provid.. |
|||
Melt Temperature | 245 - 260 °C | 473 - 500 °F | ISO 294 |
Gromax BTQ50-DQ00N1 Nylon 6, Impact Modified (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 245 - 275 °C | 473 - 527 °F | Injection Molding |
LG Chemical LUPOY GN5151RF PC/ABS Mineral Filler Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: E&E (Housing), IT/OA (Notebook PC Housing)CAS: 103598-77-2, 9003-56-9.. |
|||
Melt Temperature | 245 - 260 °C | 473 - 500 °F | |
LATI Latamid 68 H2-V0 PA6/PA66 copolymer, Heat Stabilized, Flame Retardant PA6/PA66 copolymer (PA6/PA66) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Good surface appearance.Availability: Africa & Middle Ea.. |
|||
Melt Temperature | 245 - 260 °C | 473 - 500 °F | |
Lavergne VYPET PBT 6300 BK PBT Unreinforced, Impact Modified Vypet PBT 6300 BK is an unreinforced PBT injection molding compound offering excellent dimensional stability, chemical resistance, low moisture absorption and good electrical properties.Features: Hi.. |
|||
Melt Temperature | 245 - 285 °C | 473 - 545 °F | |
Toyobo GLAMIDE® TY-102ND Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Melt Temperature | 245 - 265 °C | 473 - 509 °F | |
CP-Polymer-Technik Wellamid® 6000 HWUVCP Nylon 6, UV Stabilized, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 245 - 265 °C | 473 - 509 °F | |
CP-Polymer-Technik Wellamid® 6000 SCP Nylon 6, Finely Crystalline, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 245 - 260 °C | 473 - 500 °F | |
CP-Polymer-Technik Wellamid® 6000/42 Nylon 6, Polymer Modified, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 245 - 260 °C | 473 - 500 °F | |
CP-Polymer-Technik Wellamid® 6000/50 CP Nylon 6, Impact Modified Until 0°C, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 245 - 260 °C | 473 - 500 °F | |
CP-Polymer-Technik Wellamid® 6000/50 HWUVCP Nylon 6, Impact Modified Until 0°C, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 245 - 260 °C | 473 - 500 °F | |
Celanese Celstran® TPU-CF40-01 TPU, 40% Specialty 40% long carbon fiber reinforced Thermoplastic PolyurethaneInformation provided by Celanese |
|||
Melt Temperature | 245 - 260 °C | 473 - 500 °F | |
Celanese Celstran® TPU-GF40-01-US TPU, 40% Glass Reinforced 40% long strand glass fiber reinforced thermoplastic polyurethaneInformation provided by Celanese |