Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 1230 High Heat Crystal Polystyrene
(discontinued **) Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 1511 High Heat Crystal Polystyrene
(discontinued **) High flow and high heat resistance, Excellent clarity, USP Class VIApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 2110 General Purpose Crystal Polystyrene
(discontinued **) Moderately high heat resistance, Good balance of strength and ease of processing, USP Class VIApplications: Foam extrusion, Biaxially oriented sheet, Thermoformed drinkware, Molded packagingExposure.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 3601 General Purpose Crystal Polystyrene
(discontinued **) Easy flow for high productivity, excellent post molding scuff resistanceApplications: Medical, LabwareExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the phys.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 3700 General Purpose Crystal Polystyrene
(discontinued **) Good balance of flow and strength, Good crack resistanceApplications: Single service wares, Blending resinExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the .. |
|||
Melt Temperature | 168 - 274 °C | 335 - 525 °F | Average value: 221 °C Grade Count:17 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | Average value: 237 °C Grade Count:6 |
Overview of materials for Nylon 12, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Melt Temperature | 210 - 274 °C | 410 - 525 °F | Average value: 231 °C Grade Count:5 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Melt Temperature | 232 - 274 °C | 450 - 525 °F | Injection Molding |
Ineos ABS Lustran® 451 ABS, Injection Molding Grade Lustran® ABS 451 is a soft flowing, medium impact injection molding resin designed with a unique balance of impact, heat resistance, flow, and gloss. |
|||
Melt Temperature | 218 - 274 °C | 425 - 525 °F | |
Star Plastics ABS3030 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Melt Temperature | 218 - 274 °C | 425 - 525 °F | |
Star Plastics ABSGF30 Molding Grade ABS With 30% Glass Information provided by Star Plastics, Inc. |
|||
Melt Temperature | 243 - 274 °C | 470 - 525 °F | |
RTP Company EMI 2561 FR Polycarbonate/ABS Alloy (PC/ABS), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection - Flame Retardant |
|||
Melt Temperature | 243 - 274 °C | 470 - 525 °F | |
RTP Company EMI 2561 HF Polycarbonate/ABS Alloy (PC/ABS), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection - High Flow |
|||
Melt Temperature | 232 - 274 °C | 450 - 525 °F | |
Total PPR 6573XHC Polypropylene, Random Copolymer Film Grade Random copolymer film gradeColor - Low catalyst residuals in FINA 6573XHC result in improved color stability.Clarity/Impact - The random copolymer structure of FINA 6573XHC improves its clarity and .. |
|||
Melt Temperature | 243 - 274 °C | 470 - 525 °F | |
RTP Company ESD C 2500 Polycarbonate/ABS Alloy (PC/ABS), ESD Protection - Electrically Conductive |
|||
Melt Temperature | 243 - 274 °C | 470 - 525 °F | |
RTP Company RTP 2500 A Polycarbonate/ABS Alloy (PC/ABS), Base Resin |
|||
Melt Temperature | 243 - 274 °C | 470 - 525 °F | |
RTP Company RTP 2500 A TFE 10 UV Polycarbonate/ABS Alloy (PC/ABS), PTFE Lubricated - UV Stabilized |
|||
Melt Temperature | 243 - 274 °C | 470 - 525 °F | |
RTP Company RTP 2503 FR Polycarbonate/ABS Alloy (PC/ABS), Glass Fiber - Flame Retardant - PBDE Free - UL94 V-0 |
|||
Melt Temperature | 243 - 274 °C | 470 - 525 °F | |
RTP Company RTP 2599 X 113384 A Polycarbonate/ABS Alloy (PC/ABS); LDS Platable |
|||
Melt Temperature | 221 - 274 °C | 430 - 525 °F | |
RTP Company RTP 281 F Nylon 12 (PA), Carbon Fiber |
|||
Melt Temperature | 221 - 274 °C | 430 - 525 °F | |
RTP Company RTP 207 F Nylon 12 (PA), Glass Fiber |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 5120 High Impact Polystyrene
(discontinued **) Good balance of toughness and rigidity, Superior gloss, USP Class VIApplications: Refrigeration, Appliances, High gloss applicationsProperties were determined on injection molded specimens at 23°C .. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 5450 High Impact Polystyrene
(discontinued **) High impact, Good ESCRApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheet, Single service packagingProperties were determined on injection molded specimens at 23.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 5470 High Impact Polystyrene
(discontinued **) High impact, Good ESCR, Good printabilityApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheetProperties were determined on injection molded specimens at 23°C and.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 202W Crystal Polystyrene High Heat Extrusion Grade
(discontinued **) Excellent heat resistance, Superior melt strengthApplications: Foam insulationProperties were determined on injection molded specimens at 23° and 50% RH unless otherwise specified.Information provi.. |
|||
Melt Temperature | 243 - 274 °C | 470 - 525 °F | |
RTP Company ESD 2587 Polycarbonate/ABS Alloy (PC/ABS); Carbon Fiber - Electrically Conductive - ESD Protection |
|||
Melt Temperature | 221 - 274 °C | 430 - 525 °F | |
RTP Company RTP 200 F TFE 20 SI Nylon 12 (PA), PTFE Lubricated - Silicone Lubricated |
|||
Melt Temperature | 243 - 274 °C | 470 - 525 °F | |
RTP Company RTP 2500 A TFE 15 Polycarbonate/ABS Alloy (PC/ABS), PTFE Lubricated |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 5504 High Impact Polystyrene
(discontinued **) Good overall balance of properties, USP Class VIApplications: Audio cassettes and cartridges, Housewares, Toys, Structural foam, Machine housings, Window framesProperties were determined on injectio.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 204L Crystal Polystyrene General Purpose Grade
(discontinued **) Fast cycling, Good heat resistance, Good balance of properties and flow characteristics, Extrusion and Injection Molding Applications: General purpose injection molded itemsProperties were determin.. |