Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 218 - 302 °C | 424 - 576 °F | Injection |
Albis Plastics Polypropylene A 12 H-GK20/GF20 C , 20% Glass Bead/20% Glass Fiber
(discontinued **) Semi-crystalline Polypropylene Homopolymer (PPHP)Characteristics: Chemically Coupled Fiber; Good Dimensional StabilityApplications: Appliances, Furniture, Cases, Packaging and NoveltiesProcessing: I.. |
|||
Melt Temperature | 218 °C | 424 °F | Injection |
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Melt Temperature | 218 °C | 424 °F | Injection |
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Melt Temperature | 218 - 274 °C | 424 - 525 °F | |
Total PPR LX5 02-15 Polypropylene, Metallocene Film Resin TOTAL Petrochemicals Polypropylene LX5 02-15 is an experimental grade of isostatic polypropylene copolymer produced via TOTAL proprietary metallocene catalyst technology.Benefits. LX5 02-15 produc.. |
|||
Melt Temperature | 218 °C | 424 °F | Injection |
Lubrizol Estane® 58123 Thermoplastic Polyurethane Features: High moisture vapor transmission with low water swell and excellent low temperature and elasticity properties.Uses: Blown and flat die/cast film extrusion, injection molding and cable jack.. |
|||
Melt Temperature | 218 - 260 °C | 424 - 500 °F | |
Bapolene® 4052F Polypropylene, Blown Film Grade Bapolene PP4052F is a PP homopolymer for blown film applications. It contains slip and antiblock additives as processing aids. It offers good clarity and optical properties. This product meets FD.. |
|||
Melt Temperature | 218 - 232 °C | 424 - 450 °F | |
LNP Thermocomp® FP-VC-1003 BK8-019 Polyvinylidene Fluoride, Carbon Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Melt Temperature | 218 °C | 424 °F | Injection |
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Melt Temperature | 218 - 274 °C | 424 - 525 °F | |
Styron Magnum™ 1150 EM Acrylonitrile Butadiene Styrene (ABS) Overview: MAGNUM™ ABS resins are thermoplastic materials which provide an excellent balance to processability, impact resistance and heat resistance as imparted by the various polymer compositions... |