Total PPR LX5 02-15 Polypropylene, Metallocene Film Resin

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Total Atofina
Trade Name PPR
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPR LX5 02-15 Polypropylene, Metallocene Film Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TOTAL Petrochemicals Polypropylene LX5 02-15 is an experimental grade of isostatic polypropylene copolymer produced via TOTAL proprietary metallocene catalyst technology.Benefits. LX5 02-15 produces films with excellent heat seal performance and outstanding optical properties.FDA. LX5 02-15 is cleared for food contact under Title 21 CFR Section 177.1520(c) 3.2a.Recommended Applications. LX5 02-15 is an excellent material for use as a heat sealable layer un production of coextruded biaxially oriented films due to its good processing, excellent optics, very low extractables, low seal initiation temperature and exceptional hot tack seal strength properties.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.895 g/cc
0.895 g/cc
ASTM D1505
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 48.0 MPa
6960 psi
ASTM D638
Elongation at Break 800 %
800 %
ASTM D638
Heat Seal Strength Initiation Temperature 105 °C
221 °F
Thermal Properties Metric English Comments
Melting Point 119 °C
246 °F
DSC
Optical Properties Metric English Comments
Haze 0.30 %
0.30 %
ASTM D1003
Gloss 96 %
96 %
at 45°; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 218 - 274 °C
424 - 525 °F