Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 168 - 274 °C | 335 - 525 °F | Average value: 221 °C Grade Count:17 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 8600-85 Clear PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 8925-85 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 8940-85 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 8960-85 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 8980-85 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 9600-85 Clear PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 9915-85 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 9925-85 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 9950-85 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 9960-85 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 9980-85 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 9999-85 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 °C | 335 °F | Processing Temperature |
Teknor Apex APEX® 1008 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Melt Temperature | 168 °C | 335 °F | |
Teknor Apex APEX® 3201-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Melt Temperature | 168 °C | 335 °F | |
Teknor Apex APEX® 3300-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Food Service Applications, General Purpose, Me.. |
|||
Melt Temperature | 168 °C | 335 °F | |
Teknor Apex APEX® 3310-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Melt Temperature | 168 °C | 335 °F | |
Teknor Apex APEX® 90-A472R-60-NT Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Medical Applications, Caps, Closures, Valves/Valve Parts Appearance-ClearForms-PelletsProcessing Method-.. |
|||
Melt Temperature | 168 °C | 335 °F | |
Teknor Apex APEX® 3200-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Melt Temperature | 168 °C | 335 °F | |
Teknor Apex APEX® 3211-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Melt Temperature | 168 °C | 335 °F | |
Axiall 59996J Moldings & Extrusions Flexible PVC Injection and molding compound with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 168 °C | 335 °F | |
Axiall 11600 Wire & Cable Flexible PVC Clear, non-staining speaker wire insulation and general purpose extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 168 °C | 335 °F | |
Axiall 1651 Clear 7002 Flexible PVC Flexible polyvinyl chloride compound formulated for USP Class VI applications. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation .. |
|||
Melt Temperature | 168 °C | 335 °F | |
Axiall 8552 Moldings & Extrusions Flexible PVC A soft extrusion compound recommended for profiles, weatherstrips and sheeting. Also suitable for injection molding.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 201.. |
|||
Melt Temperature | 168 °C | 335 °F | |
Axiall 8651 Moldings & Extrusions Flexible PVC A quality, low gravity extrusion compound with excellent low temperature properties. Designed for use in weatherstrips, flexible gaskets and extruded shapes.Information provided by Georgia GulfGeor.. |
|||
Melt Temperature | 168 °C | 335 °F | |
Axiall 10705 Wire & Cable Flexible PVC Non-lead stabilized general purpose 75C compound with good low temperature properties. Formulated for increased line speed and reduced surface gloss.Information provided by Georgia GulfGeorgia Gulf.. |
|||
Melt Temperature | 168 °C | 335 °F | |
Axiall 10757 Wire & Cable Flexible PVC General purpose non-lead stabilized 75°C rated compound recommended for jacketing and general purpose extrusion applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporati.. |
|||
Melt Temperature | 168 °C | 335 °F | |
Teknor Apex APEX® 3202-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Caps, Closure, Connectors, Food Service Applications, Safety Equipment, Valves/Valve Parts Appearance-Cl.. |
|||
Melt Temperature | 168 °C | 335 °F | |
Teknor Apex APEX® 3311-60NT Polyvinyl Chloride, Flexible Features: Non-DEHP Plasticizer; Ethylene Oxide Sterilizable Uses: Medical/Healthcare Applications; Toys; Tubing Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor Apex |
|||
Melt Temperature | 168 °C | 335 °F | |
Axiall 22750 Coax & Telecom Flexible PVC Non-staining extrusion compound recommended for retractile telecommunication cord. Maximum service temperature of 60°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in.. |