Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 246 - 274 °C | 475 - 525 °F | |
Polymer Resources PC/ABS-FR1-[color]-UV Flame Retardant PC/ABS Alloy, UV-stabilized PC/ABS Alloy, Flame Retardant, Standard Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 1511 High Heat Crystal Polystyrene
(discontinued **) High flow and high heat resistance, Excellent clarity, USP Class VIApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 1531 High Heat Crystal Polystyrene
(discontinued **) High flow and high heat resistance, Excellent clarityApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and optical p.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 2580 General Purpose Crystal Polystyrene
(discontinued **) High speed molding, Improved crack resistanceApplications: Cutlery, Consumer electronicsExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and optic.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 3504 General Purpose Crystal Polystyrene
(discontinued **) Good blending resin, Suitable for difficult to fill an thin wall molding, USP Class VIApplications: Cosmetic and medical packaging, Housewares, Consumer Electronic packaging, ToysExposure to gamma r.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 1600 High Heat Crystal Polystyrene High heat resistance, Moderate flow, Good balance of strength and set-upApplications: Foam extrusion, Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant e.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 5404 High Impact Polystyrene High impact, Good environmental stress crack resistance, USP Class VIApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheet, Single service packagingProperties were.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 5410 High Impact Polystyrene High impact, Good ESCR, Good printabilityApplications: Thermoformed containers and lids, Hot and cold beverages cups, Custom sheetProperties were determined on injection molded specimens at 23°C .. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova FX530 Impact Polystyrene Features: Excellent environmental stress crack resistanceExcellent Izod impact strengthUL Classification 94 HBBalanced physical propertiesApplications: ExtrusionThermoformingSelected injection moldi.. |
|||
Melt Temperature | 218 - 274 °C | 425 - 525 °F | |
Star Plastics ABS3545 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Melt Temperature | 232 - 274 °C | 450 - 525 °F | oriented film extrusion |
Total PPH 3276 Polypropylene, Oriented Film Extrusion Grade Homopolymer film gradeLow Residuals – Fina 3276 utilizes the new Fina proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblock .. |
|||
Melt Temperature | 268 - 274 °C | 514 - 525 °F | |
LNP Lubricomp® IBL-4416 Polyamide 6/12 Copolymer, Glass Bead Reinforced, Silicone Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 3511 General Purpose Crystal Polystyrene
(discontinued **) Excellent blending resin, Suitable fore difficult to fill and thin wall molding, USP Class VIApplications: Single service cutlery, Cosmetic and medical molding, Consumer electronic packagingExposure.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 5420 High Impact Polystyrene
(discontinued **) High impact, Good environmental stress crack resistance, USP Class VIApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheetProperties were determined on injection m.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 5450 High Impact Polystyrene
(discontinued **) High impact, Good ESCRApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheet, Single service packagingProperties were determined on injection molded specimens at 23.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 6260 Super High Impact Polystyrene
(discontinued **) Good toughness, Deep draw, Easy processing using all conventional methodsApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 201 Crystal Polystyrene High Heat Extrusion Grade
(discontinued **) Excellent heat resistance, Superior melt strengthApplications: Foam insulation, Oriented polystyrene sheet (OPS), XPS food packaging, Sheet and profile extrusionProperties were determined on injecti.. |
|||
Melt Temperature | 246 - 274 °C | 475 - 525 °F | |
Polymer Resources PPX-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 5504 High Impact Polystyrene
(discontinued **) Good overall balance of properties, USP Class VIApplications: Audio cassettes and cartridges, Housewares, Toys, Structural foam, Machine housings, Window framesProperties were determined on injectio.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 610 Crystal Polystyrene GP Grade
(discontinued **) Broad, medium melt flow range, Broad Vicat rangeApplications: Any; Injection Molding and ExtrusionProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise spe.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 6110 Super High Impact Polystyrene
(discontinued **) Good balance of gloss and impact, High glossApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined on injection molded specimen.. |