Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Hytrel® HTR8730 BK320 TPC-ET  (Unverified Data**)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyester Thermoplastic Elastomer
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Hytrel® HTR8730 BK320 TPC-ET  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hytrel® HTR8730 BK320 is a high viscosity thermoplastic polyester elastomer designed for blow molding. It has excellent mechanical properties at elevated temperatures and very good resistance to most automotive fluids.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Water Absorption 0.30 %

@Temperature 23.0 °C
0.30 %

@Temperature 73.4 °F
Immersion 24h; ISO 62, Similar to
Melt Flow 6.0 g/10 min

@Load 10.0 kg,
Temperature 230 °C
6.0 g/10 min

@Load 22.0 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 60

@Time 15.0 sec
60

@Time 0.00417 hour
ISO 868
Tensile Strength at Break 41.0 MPa

@Temperature 23.0 °C
5950 psi

@Temperature 73.4 °F
ISO 527 (1BA bar)
Tensile Stress 10.0 MPa

@Strain 5.00 %,
Temperature 23.0 °C
1450 psi

@Strain 5.00 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
15.0 MPa

@Strain 10.0 %,
Temperature 23.0 °C
2180 psi

@Strain 10.0 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
Elongation at Break 340 %

@Temperature 23.0 °C
340 %

@Temperature 73.4 °F
ISO 527 (1BA bar)
Tensile Modulus 0.273 GPa

@Temperature 23.0 °C
39.6 ksi

@Temperature 73.4 °F
ISO 527
Charpy Impact, Notched 1.00 J/cm²

@Temperature -40.0 °C
4.76 ft-lb/in²

@Temperature -40.0 °F
ISO 179/1eA
1.40 J/cm²

@Temperature -30.0 °C
6.66 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 212 °C
414 °F
10°C/min; ISO 11357-1/-3
Processing Properties Metric English Comments
Melt Temperature 230 °C
446 °F
Optimum; Blow Molding
230 °C
446 °F
Optimum; Extrusion
225 - 235 °C
437 - 455 °F
Blow Molding
225 - 235 °C
437 - 455 °F
Extrusion
Drying Temperature 100 °C
212 °F
Blow Molding
100 °C
212 °F
Extrusion
Dry Time 2.00 - 3.00 hour
2.00 - 3.00 hour
Blow Molding
2.00 - 3.00 hour
2.00 - 3.00 hour
Extrusion
Moisture Content <= 0.030 %
<= 0.030 %
Blow Molding
<= 0.050 %
<= 0.050 %
Extrusion
Descriptive Properties Value Comments
Forms Pellets
Generic TPC-ET
Material Status Preliminary Data
Part Marking Code >TPC-ET<
ISO 11469
Processing Method Blow Molding
Product Category Blow Moldable Resins
Region Available - Global Yes
Resin Identification TPC-ET
ISO 1043
RoHS Compliance Contact Manufacturer
Users viewing this material also viewed the following: