Polymer Property : Melt Temperature = 165 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Wire & Cable E 1400 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Wire & Cable E1330I Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Wire & Cable EC486 DA Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Wire & Cable JC837DB Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Wire & Cable L00221 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Wire & Cable WJCK504L Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Wire & Cable WR8180L Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 165 - 175 °C
329 - 347 °F
Petroquimica Triunfo Trithene® SX 7012 LDPE - Blow Molding
The Trithene SX 7012 resin is a low density polyethylene (LDPE) with medium molecular weight which allows the production of flasks with an adequate combination of mechanical and impact strength, fle..
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Flexible R7543E Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Flexible R7545H Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Flexible R7661A Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Flexible R7831A Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Flexible R8180K Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 165 - 235 °C
329 - 455 °F
M. Holland Company MAGMA® Magmalene Polyalphaolefin  (discontinued **)
High Clarity, Good Flexibility, Good Flow, High Gloss, Good ToughnessUses: BlendingProcessing Method: Injection MoldingInformation provided by M. Holland.
Melt Temperature 165 - 235 °C
329 - 455 °F
M. Holland Company MAGMA® LM372-A LLDPE  (discontinued **)
Features: High Clarity, Good Flexibility, Good Flow, High Gloss, Good ToughnessProcessing Method: Injection MoldingInformation provided by M. Holland.
Melt Temperature 165 °C
329 °F
Molding
PolyOne Edgetek® GF 5209 10 FPS 15 BLACK 30 A 1 Acetal-Copolymer, Glass Filled  (discontinued **)
PRELIMINARY DATA SHEETDescription/Features:Glass Fiber ReinforcedBlackInformation provided by PolyOne Corporation.
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Flexible R3792C Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Flexible R3792E Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Flexible R8206A Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 165 - 175 °C
329 - 347 °F
Lucobit Lucofin® 7410 HFFR EBA MDH Cable Sheathing
Lucofin® 7410 HFFR is a thermoplastic, halogen free flame retardant and low smoke compound for the insulation and/ or sheathing of cables. This grade is based on ethylene butyl acrylate (EBA) and..
Melt Temperature 165 - 170 °C
329 - 338 °F
Metabolix Mirelâ„¢ P4001 Sheet Extrusion Grade Bioplastic
Mirelâ„¢ P4001 is a general purpose, high melt strength material suitable for cast sheet extrusion. Mirelâ„¢ P4001 is designed for a wide range of sheet applications including gift cards, prom..
Melt Temperature 165 - 200 °C
329 - 392 °F
Borealis Bormed™ LE6607-PH LDPE for Pharmaceutical Blow Molding
Bormed LE6607-PH is a LD-polyethylene produced in a high pressure process intended for blow molding of sot and flexible packages for pharmaceutical products.Bormed LE6607-PH can be used in "blow-fil..
Melt Temperature 165 - 200 °C
329 - 392 °F
Borealis Bormed™ LE6609-PH LDPE for Pharmaceutical Blow Molding
Bormed LE6609-PH is a LD-polyethylene produced in a high-pressure process intended for blow molding of soft and flexible packages for pharmaceutical products.Bormed LE6609-PH can be used in "blow-fi..
Melt Temperature 165 - 175 °C
329 - 347 °F
EMS-Griltech Grilene® KE 170 CoPES Mono-Component Fusible Adhesive Fiber
Description: Grilene KE 170 is the higher melting CoPES mono-component fusible adhesive fiber. It is used in compact dry-laid nonwoven.Data provided by EMS-Griltech.
Melt Temperature 165 - 185 °C
329 - 365 °F
Blow Film Extrusion
Braskem TN2020 EVA General Film Copolymer
TN2020 is an Ethylene-Vinyl Acetate (EVA) copolymer developed to mostly meet the needs of the multi-layer packaging segment produced by coextrusion and/or lamination processes. Multilayer structures..
Melt Temperature 165 - 205 °C
329 - 401 °F
Huntsman Rexell® V8401 Cast Film Extrusion LLDPE  (discontinued **)
Ultra linear-low density copolymer, blown film extrusion, FDA compliant.Features: Excellent combination of flexibility, flex crack resistance, and low temperature properties. It also exhibits excell..
Melt Temperature 165 - 205 °C
329 - 401 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1035D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical
Melt Temperature 165 - 205 °C
329 - 401 °F
Injection Molding
LG Chemical KEYFLEX BT 1035D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical