Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

M. Holland Company MAGMA® Magmalene Polyalphaolefin  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded , Polyolefin
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company MAGMA® Magmalene Polyalphaolefin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Clarity, Good Flexibility, Good Flow, High Gloss, Good ToughnessUses: BlendingProcessing Method: Injection MoldingInformation provided by M. Holland.
Physical Properties Metric English Comments
Density 0.870 g/cc
0.0314 lb/in³
ASTM D1505
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ASTM D2240
Film Tensile Strength at Yield, MD 1.31 MPa
190 psi
ASTM D882
Film Elongation at Break, MD >= 1000 %
>= 1000 %
ASTM D882
Flexural Modulus 0.0165 GPa
2.40 ksi
2% Secant, in accordance with ASTM D638; ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 41.1 °C
106 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 165 - 235 °C
329 - 455 °F
Mold Temperature 50.0 - 60.0 °C
122 - 140 °F
Injection Pressure 10.0 - 14.0 MPa
1450 - 2030 psi
Descriptive Properties Value Comments
Form Pellets
Injection Rate Fast
Users viewing this material also viewed the following: