Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eastman Eastalloy MA510 Polymer  (discontinued **)

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/PET Polyester Blend , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Eastalloy MA510 Polymer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Eastalloy MA510 Polymer is a clear copolyester/polycarbonate alloy. It affords the consumer excellent impact strength, chemical resistance, dimensional stability, low shrinkage rates and other enhanced physical properties advantages.Applications/UsesMedicalMedical DevicesKey AttributesGood chemical resistanceGood ClaritySterilizable with ethylene oxide, electron beam, and gamma raysWide range of clear tints and opaque colorsElevated in-use temperature resistanceHeat resistanceTough, excellent impact strength
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Water Absorption 0.15 %
0.15 %
24h Immersion; ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 56.0 MPa
8120 psi
ASTM D638
Tensile Strength, Yield 50.0 MPa
7250 psi
ASTM D638
Elongation at Break 195 %
195 %
ASTM D638
Elongation at Yield 5.5 %
5.5 %
ASTM D638
Flexural Strength 76.0 MPa
11000 psi
ASTM D790
Flexural Modulus 2.10 GPa
305 ksi
ASTM D790
Izod Impact, Notched 0.910 J/cm

@Temperature -40.0 °C
1.70 ft-lb/in

@Temperature -40.0 °F
ASTM D256
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D4812
NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
ASTM D4812
Puncture Energy 55.0 J
40.6 ft-lb
Puncture Resistance @Max Load, 23°C; ASTM D3763
49.0 J

@Temperature -40.0 °C
36.1 ft-lb

@Temperature -40.0 °F
Puncture Resistance at Max Load; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C
171 °F
ASTM D648
Optical Properties Metric English Comments
Haze 0.50 %
0.50 %
ASTM D1003
Transmission, Visible 86 %
86 %
Total Transmittance; ASTM D1003
Processing Properties Metric English Comments
Melt Temperature 266 - 288 °C
511 - 550 °F
Mold Temperature 27.0 - 60.0 °C
80.6 - 140 °F
Drying Temperature 88.0 °C
190 °F
Dry Time 4 - 6 hour
4 - 6 hour