Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 266 - 293 °C | 511 - 559 °F | |
PolyOne Gravi-Tech™ GRV-NY-035-SS-GF-BLK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Melt Temperature | 266 - 299 °C | 511 - 570 °F | Blow Molding |
PolyOne OnColor™ F Polyester, Thermoplastic (Polyester, TP) Information provided by PolyOne |
|||
Melt Temperature | 266 - 282 °C | 511 - 540 °F | |
PolyOne Edgetek® TR2-30GF/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Melt Temperature | 266 - 282 °C | 511 - 540 °F | |
PolyOne Edgetek® X TR2-10GF/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Melt Temperature | 266 - 282 °C | 511 - 540 °F | |
PolyOne Edgetek® X TR2-10TA/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Melt Temperature | 266 - 282 °C | 511 - 540 °F | |
PolyOne Edgetek® X TR2-20GF/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Melt Temperature | 266 - 282 °C | 511 - 540 °F | |
PolyOne Edgetek® X TR2-20TA/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Melt Temperature | 266 - 282 °C | 511 - 540 °F | |
PolyOne Edgetek® X TR2-30TA/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Melt Temperature | 266 - 288 °C | 511 - 550 °F | |
Eastman Eastalloy DA510 Polymer
(discontinued **) Eastalloy Polymer DA510 is a clear copolyester/polycarbonate alloy. This product has good physical properties. These include good impact strength, chemical resistance, heat resistance, dimensional s.. |
|||
Melt Temperature | 266 - 288 °C | 511 - 550 °F | |
Eastman Eastalloy MA510 Polymer
(discontinued **) Eastalloy MA510 Polymer is a clear copolyester/polycarbonate alloy. It affords the consumer excellent impact strength, chemical resistance, dimensional stability, low shrinkage rates and other enhan.. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax BFM30-EL03N1 Nylon 6 30% Mineral Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax BFM30-EL03N1 Nylon 6 30% Mineral Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax BFM30-EL04B2 Nylon 6 30% Mineral Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax BFM30-EL04B2 Nylon 6 30% Mineral Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax BFM40-DL04N1 Nylon 6 40% Mineral Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax BFM40-DL04N1 Nylon 6 40% Mineral Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax CFG33-RN13N1 Nylon 6 33% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax CFG35-R113N1 Nylon 6 36% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax CFG45-PN11N1 Nylon 6 46% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax CFG45-PN11N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax CFG45-RN13N1 Nylon 6 46% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 °C | 511 °F | |
Chem Polymer Chemlon 109 Nylon 66, High Impact A highly impact-modified, lubricated nylon 66 exhibiting excellent toughness, especially at lower temperatures.Data provided by the manufacturer, Chem Polymer. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax CFG30-QN11N1 Nylon 6 30% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax CFG30-SN31N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax CFG30-QN11N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax CFG30-SN31N1 Nylon 6 30% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax CFG33-RN13N1 Nylon 6 33% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax CFG35-R113N1 Nylon 6 36% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax CFG45-RN13N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |