Entec Hylex® P1025G10NHFR Polycarbonate, 10% Glass Reinforced

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Entec Engineered Resins
Trade Name Hylex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Entec Hylex® P1025G10NHFR Polycarbonate, 10% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Entec.
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Water Absorption 0.14 %
0.14 %
24-Hr Immersion; ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
ASTM D955
Melt Flow 22 - 28 g/10 min

@Load 3.80 kg,
Temperature 230 °C
22 - 28 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 79.3 MPa
11500 psi
ASTM D638
Elongation at Break 2.2 %
2.2 %
ASTM D638
Flexural Strength 114 MPa
16500 psi
ASTM D790
Flexural Modulus 4.14 GPa
600 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm

@Thickness 3.17 mm
2.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 132 °C
270 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 128 °C
262 °F
ASTM D648
Vicat Softening Point 149 °C
300 °F
ASTM D1525
Flammability, UL94 V-0
V-0
0.071 inches
Processing Properties Metric English Comments
Rear Barrel Temperature 260 - 277 °C
500 - 530 °F
Middle Barrel Temperature 266 - 277 °C
510 - 530 °F
Front Barrel Temperature 271 - 282 °C
520 - 540 °F
Nozzle Temperature 277 - 288 °C
530 - 550 °F
Melt Temperature 277 - 288 °C
530 - 550 °F
Mold Temperature 71.1 - 93.3 °C
160 - 200 °F
Drying Temperature 110 - 121 °C
230 - 250 °F
Dry Time 3 - 4 hour
3 - 4 hour
4 - 6 hour
4 - 6 hour
with regrind
Injection Pressure 5.52 - 11.0 MPa
800 - 1600 psi
Hold Pressure 5.52 - 8.27 MPa
800 - 1200 psi
Back Pressure 0.345 - 0.689 MPa
50.0 - 100 psi
Shot Size 40 - 60 %
40 - 60 %
To Cylinder
Screw Speed 40 - 70 rpm
40 - 70 rpm