Material Notes:
High flow reactor grade homopolymer for nonwoven fibersHigh Purity - FINA 3860X features extremely high purity for processing in micro denier fibers.FDA - FINA 3860X complies with all applicable FDA regulations for food contact applications.Recommended Applications - FINA 3860X is recommended for nonwoven fiber applications.Processing - FINA 3860X resin processes on conventional extrusion equipment with typical melt temperatures of 450-550°F (232-288°C)Data provided by the manufacturer, Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D1505
Melt Flow 100 g/10 min
100 g/10 min
ASTM D1238L
Mechanical Properties Metric English Comments
Modulus of Elasticity 1.655 GPa
240.0 ksi
ASTM D638
Flexural Modulus 1.517 GPa
220.0 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
DSC
Processing Properties Metric English Comments
Melt Temperature 232 - 288 °C
450 - 550 °F
Extrusion
Users viewing this material also viewed the following: