Ecomass® 1050ZB92 Filled Polyamide

Category Polymer , Thermoplastic , Nylon
Manufacturer Ecomass Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ecomass® 1050ZB92 Filled Polyamide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nontoxic alternative to Lead (Pb), radiation shielding applications.Moderate Specific GravityFilled Polyamide (PA) alloyGood ToughnessInformation provided by Technical Polymers
Physical Properties Metric English Comments
Specific Gravity 6.90 g/cc
6.90 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0060 cm/cm
0.0050 - 0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 44.8 MPa
6500 psi
ASTM D638
Elongation at Break 1.75 %
1.75 %
ASTM D638
Tensile Modulus 6.21 GPa
900 ksi
ASTM D638
Flexural Strength 48.3 MPa
7000 psi
ASTM D790
Flexural Modulus 4.96 GPa
720 ksi
ASTM D790
Izod Impact, Notched 1.12 J/cm
2.10 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 121 °C
250 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 107 °C
225 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 232 - 260 °C
450 - 500 °F
Mold Temperature 65.6 - 82.2 °C
150 - 180 °F
Drying Temperature 73.9 °C
165 °F
Dry Time 4 hour
4 hour