Total PPH 3576XHD Polypropylene Homopolymer, Film Grade

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Total Atofina
Trade Name PPH
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPH 3576XHD Polypropylene Homopolymer, Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low Residuals TOTAL Polypropylene 3576XHD utilizes the new ATOFINA proprietary process technology to provide extremely low residuals for improved color stability and clarity.Antiblock. 3576XHD is formulated with a special antiblock additive.FDA. 3576XHD complies with all applicable FDA regulations for food contact applications.Recommended Applications. TOTAL Polypropylene 3576XHD is recommended for use in non-oriented cast film processes for manufacture of packaging films.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
ASTM D1505
Water Vapor Transmission 18.6 g/m²/day

@Temperature 37.8 °C
1.20 g/100 in²/day

@Temperature 100 °F
90% RH; ASTM F1249-90
Melt Flow 9.0 g/10 min
9.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.2 MPa
8000 psi
ASTM D882
Elongation at Break 500 %
500 %
ASTM D882
Secant Modulus 0.793 GPa
115 ksi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 163 °C
325 °F
DSC
Optical Properties Metric English Comments
Haze 5.0 %
5.0 %
ASTM D1003
Gloss 75 %
75 %
at 45°; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 232 - 274 °C
450 - 525 °F
Cast Film Extrusion