Iran Petrochemical (PCC) LH0075 Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Blow Molding Grade , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) LH0075 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LH0075 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Applications: carrier bags, shrink film, industrial film, dust bin liners, large bottles, blow molding of small container, packaging of pharmaceutical products.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
TSTM 209 B
Melt Flow 0.75 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.75 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Stress 16.7 MPa
2420 psi
at Break, MD; ASTM D882
Elongation at Break >= 300 %
>= 300 %
ASTM D882, MD
>= 450 %
>= 450 %
ASTM D882, TD
Dart Drop Test 120 g
0.265 lb
ASTM D1709
Thermal Properties Metric English Comments
Vicat Softening Point 94.0 °C
201 °F
ASTM D1525
Heat Distortion Temperature 33.0 °C
91.4 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 180 - 210 °C
356 - 410 °F