Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Advanced Polymer Alloys DuraGrip™ 6140 NC Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer APA - Advanced Polymer Alloys
Trade Name DuraGrip™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Advanced Polymer Alloys DuraGrip™ 6140 NC Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DuraGrip® 6140NC is an enhanced bonding and adhesion grade Thermoplastic Elastomer (TPE) designed for injection molding and extrusion processes. It will bond well with polycarbonate, polycarbonate alloys, ABS, ASA, acrylics, cellulosics, and some nylons in insert molding, co-injection molding and coextrusion processes. DuraGrip® 6140NC is hygroscopic and requires drying at 150°F for 3-4 hours for optimum aesthetics, properties and adhesion.Information provided by Advanced Polymer Alloys
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
ASTM D471
Viscosity 374000 cP

@Shear Rate 294 1/s,
Temperature 190 °C
374000 cP

@Shear Rate 294 1/s,
Temperature 374 °F
ASTM D3835
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
5 Sec; ASTM D2240
Tensile Strength at Break 2.96 MPa
430 psi
ASTM D412
Elongation at Break 410 %
410 %
ASTM D412
100% Modulus 0.00117 GPa
0.170 ksi
ASTM D412
300% Modulus 0.00207 GPa
0.300 ksi
ASTM D412
Graves Tear Strength 16.5 kN/m

@Temperature 24.0 °C
94.0 pli

@Temperature 75.2 °F
Die C; ASTM D624
Processing Properties Metric English Comments
Melt Temperature 180 - 230 °C
356 - 446 °F
Users viewing this material also viewed the following: