Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis Borstar® HE 6068 Natural Bimodal HDPE with very low shrinkage for Submarine and Fiber Optical Cables

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Borealis
Trade Name Borstar®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Borstar® HE 6068 Natural Bimodal HDPE with very low shrinkage for Submarine and Fiber Optical Cables.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Borstar® HE6068 is a natural, UV-stabilized, colorable, bimodal high density (HD) jacketing compound, which is produced with the Borealis proprietary Borstar® bimodal process technology. Borstar® technology allows the manufacturing of polymers outside the traditional MFR and density range making it possible to optimize processability, reduce shrinkage and yet provide excellent physical toughness and environmental stress crack resistance (ESCR). Borstar® HE6068 contains a well dispersed UV-stabilizer in sufficient amount providing a measure of weathering resistance. Applications: Borstar® HE6068 is designed for Submarine and fibre optical cables Borstar® HE6068 offers substantially reduced shrinkage which helps to maintain low signal attenuation for fibre optic communication cables and low jacket retraction for energy cables in combination with excellent mechanical and barrier properties. Borstar® HE6068 offers a balance of properties giving advantages in manufacturing, installation and lifetime performance of communication and energy cables. Specifications Borstar® HE6068 meets the applicable requirements as below when processed using sound extrusion practice and testing procedure: ASTM D 1248 Type III, Class A, Category 3, Grade E8, E9, J4, BS 6234: Type H2, TS2, DIN 57818/VDE 0818, HD 620 S1, Part 1, table 4B, DMP 5, 13, 16, IEC 60502, Type ST7, IEC 60840, Type ST7, and ISO 1872-PE, KHLN, 45 D-022.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.944 g/cc
0.0341 lb/in³
ISO 1183/ISO 1872-2
Environmental Stress Crack Resistance >= 5.0 hour

@Temperature 50.0 °C
>= 5.0 hour

@Temperature 122 °F
Igepal 10%;F0; IEC 60811-4-1/B
Melt Flow 1.7 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.7 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
3s; ISO 868
61
61
1s; ISO 868
Tensile Strength, Yield 31.0 MPa
4500 psi
50mm/min; ISO 527
Elongation at Break 900 %
900 %
50mm/min; ISO 527
Flexural Modulus 0.850 GPa
123 ksi
ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -76.0 °C
<= -105 °F
ASTM D746
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+6 ohm-cm
1.00e+6 ohm-cm
DC; IEC 60093
Dielectric Strength 70.0 kV/mm
1780 kV/in
IEC 60243
Processing Properties Metric English Comments
Processing Temperature 90.0 °C
194 °F
preheating temperature
Melt Temperature 180 - 190 °C
356 - 374 °F
Die Cooling Temperature 60.0 °C
140 °F
cooling water
Descriptive Properties Value Comments
High Temperature Pressure Test, % < 10%
115°C; 6 hours; IEC 60811-3-1
Users viewing this material also viewed the following: