Lubrizol ESTANE® 58866 Ether Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 58866 Ether Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Transparent flame retardant compoundUses: Extrusion – Wire and cable, Hose and tubeAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ASTM D792
Loss On Ignition 30 %
30 %
ASTM D2863
Maximum Moisture Content 0.020
0.020
Mechanical Properties Metric English Comments
Hardness, Shore A 82 - 88

@Time 5.00 sec
82 - 88

@Time 0.00139 hour
ASTM D2240
Tensile Strength 27.6 MPa
4000 psi
ASTM D412
Elongation at Break 730 %
730 %
ASTM D412
100% Modulus 0.00450 GPa
0.653 ksi
ASTM D412
300% Modulus 0.00690 GPa
1.00 ksi
ASTM D412
Flexural Modulus 0.0229 GPa
3.32 ksi
ASTM D790
Tear Strength 18.4 kN/m
105 pli
Trouser; ASTM D470
Graves Tear Strength 54.3 kN/m
310 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 3.0
3.0
CS-17, 1000g; ASTM D3389 B
Compression Set 24 %

@Temperature 23.0 °C,
Time 79200 sec
24 %

@Temperature 73.4 °F,
Time 22.0 hour
70 %

@Temperature 70.0 °C,
Time 79200 sec
70 %

@Temperature 158 °F,
Time 22.0 hour
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -47.0 °C
-52.6 °F
DSC
Flammability, UL94 V-0
V-0
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Zone 1 177 °C
351 °F
Extrusion
Zone 2 183 °C
361 °F
Extrusion
Zone 3 188 °C
370 °F
Extrusion
Zone 4 194 °C
381 °F
Extrusion
Adapter Temperature 194 °C
381 °F
5, Extrusion
Die Temperature 185 °C
365 °F
Zone 2, Extrusion
191 °C
376 °F
6, Zone 1, Extrusion
Drying Temperature 104 °C
219 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Dew Point -40.0 °C
-40.0 °F