Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol ESTANE® 58284 Ether Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 58284 Ether Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Matte finish, superior durabilityUses: Extrusion – wire and cable, General applicationAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Maximum Moisture Content 0.020
0.020
Mechanical Properties Metric English Comments
Hardness, Shore A 82 - 88

@Time 5.00 sec
82 - 88

@Time 0.00139 hour
ASTM D2240
Tensile Strength 48.3 MPa
7010 psi
ASTM D412
Elongation at Break 550 %
550 %
ASTM D412/D638
100% Modulus 0.00700 GPa
1.02 ksi
ASTM D412
300% Modulus 0.0131 GPa
1.90 ksi
ASTM D412
Tear Strength 12.4 kN/m
71.0 pli
Trouser; ASTM D470
Graves Tear Strength 167 kN/m
950 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 83
83
H-18, 1000g; ASTM D3389 B
Compression Set 19 %

@Temperature 23.0 °C,
Time 79200 sec
19 %

@Temperature 73.4 °F,
Time 22.0 hour
68 %

@Temperature 70.0 °C,
Time 79200 sec
68 %

@Temperature 158 °F,
Time 22.0 hour
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -44.0 °C
-47.2 °F
Processing Properties Metric English Comments
Zone 1 174 °C
345 °F
Extrusion
Zone 2 179 °C
354 °F
Extrusion
Zone 3 185 °C
365 °F
Extrusion
Zone 4 191 °C
376 °F
Extrusion
Adapter Temperature 191 °C
376 °F
Extrusion
Die Temperature 179 °C
354 °F
Zone 2, Extrusion
185 °C
365 °F
Zone 1, Extrusion
Drying Temperature 104 °C
219 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Dew Point -40.0 °C
-40.0 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved