Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PC/TP-GP2 PC/Polyester Alloy High Impact, Excellent Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b.. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PC/TP-GP2-G10 PC/Polyester Alloy, 10% Glass Reinforced Excellent Chemical Resistance, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p.. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PC/TP-GP3-G20 PC/Polyester Alloy, 20% Glass Reinforced Superior Chemical Resistance, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PC/TP-GP3-G30 PC/Polyester Alloy, 30% Glass Reinforced Superior Chemical Resistance, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PC/TP-GP3-IM PC/Polyester Alloy, Impact Modified Superior Chemical Resistance, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide.. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PPX-EN-FR3 Modified-PPO, V-1 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PPX-FR3-[color]EN Modified PPO, UL 94 V-1 with HDT of 265 F, Extrusion Grade Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PPX-FRG10 Modified-PPO, V-1 Flame Retardant, 10% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 10% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PPX-G30 Modified-PPO, 30% Glass Reinforced Modified-Polyphenylene Oxide, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PPX-GP3-[color]-EN Modified-PPO, Extrusion Grade Modified-Polyphenylene Oxide, Extrusion Grade, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: ExtrusionNotes: All physical, mechanical and thermal testing conduct.. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PPX-GP5 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 270F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PPX-GP7 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 300F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PPX-MF-FR3 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced Modified-Polyphenylene Oxide, V-0 Flame Retardant, 230F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha.. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PPX-MF-FRG20 Modified-PPO, 40% Glass/Mineral Reinforced, Flame Retardant Modified-Polyphenylene Oxide, 40% Glass/Mineral Reinforced, Flame RetardantFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanica.. |
|||
Drying Temperature | 104 °C | 220 °F | |
Ravago Manufacturing Americas Hybrid S464 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Drying Temperature | 104 °C | 220 °F | |
PTS PCA-1010HF High Flow Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 104 °C | 220 °F | |
PTS PCA-1012 High Impact Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 104 °C | 220 °F | |
PolyOne Edgetek® PS-15GF/000 FR Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 104 °C | 220 °F | |
PolyOne Edgetek® PS-25MN/000 Polybutylene Terephthalate (PBT), Mineral Filled
(discontinued **) Description/Features:Mineral FilledUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PC/TP-GP2-G20 PC Polyester, Excellent Chemical Resistance, 20% Glass Filled
(Unverified Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PPX-GP1 Modified PPO, General Purpose with HDT of 265 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PPX-GP3 Modified PPO, General Purpose with HDT of 235 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 104 - 110 °C @Time 7200 - 14400 sec |
220 - 230 °F @Time 2.00 - 4.00 hour |
|
Ravago Manufacturing Americas Hybrid S464LG Acrylonitrile Butadiene Styrene + PC Alloy Available in North America Good Toughness Low Gloss RoHS Compliant Form: Pellets Processing Method: Injection Molding Automotive Specifications: Chrysler MS-DB300 CPN4352 Color: Natural, Chry.. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
LTL Color Compounds ColorFast® PAHF Polycarbonate-ABS Alloy General purpose HB-rated PC/ABS with improved chemical resistanceAll information provided by LTL Color Compounders, Inc. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PPX-G10 Modified PPO, 10% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PPX-G20 Modified PPO, 20% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PPX-G30 Modified PPO, 30% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PPX-GP6 Modified PPO, General Purpose with HDT of 290 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PPX-MF-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F, Mineral Reinforced
(Unverified Da Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |