Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Green Dot Terratek® SC 65 Polypropylene - Wheat Starch Biocomposite

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Green Dot Holdings
Trade Name Terratek®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Green Dot Terratek® SC 65 Polypropylene - Wheat Starch Biocomposite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Terratek® SC 65 is a proprietary blend of wheat starch and polypropylene for injection molding applications. SC 65 contains 65% wheat starch by weight, however, a range of properties can be achieved by altering the starch to plastic ratio and by the inclusion or admission of other additives. Formulations containing anywhere from 30% to 65% starch are available upon request. Terratek® SC can be injection molded or extruded using standard processing machinery. Information provided by Green Dot Holdings.
Physical Properties Metric English Comments
Bulk Density 0.641 - 0.721 g/cc
0.0231 - 0.0260 lb/in³
Density 1.23 g/cc
0.0444 lb/in³
Moisture Absorption <= 1.00 %
<= 1.00 %
Mechanical Properties Metric English Comments
Tensile Strength at Break 26.0 MPa
3770 psi
Processing Properties Metric English Comments
Rear Barrel Temperature 177 - 182 °C
350 - 360 °F
Middle Barrel Temperature 177 - 182 °C
350 - 360 °F
Front Barrel Temperature 182 - 191 °C
360 - 375 °F
Nozzle Temperature 182 - 191 °C
360 - 375 °F
Melt Temperature <= 204 °C
<= 400 °F
Mold Temperature 15.6 - 76.7 °C
60.0 - 170 °F
Drying Temperature 104 °C
220 °F
desiccant dryer
Moisture Content <= 0.50 %
<= 0.50 %
Users viewing this material also viewed the following: