Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol ESTANE® 58370 Ether Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 58370 Ether Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Halogenated flame retardant compoundUses: Extrusion – Wire and cable and general application where flame retardant properties are neededAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Loss On Ignition 28 %
28 %
ASTM D2863
Maximum Moisture Content 0.020
0.020
Mechanical Properties Metric English Comments
Hardness, Shore A 77 - 83

@Time 5.00 sec
77 - 83

@Time 0.00139 hour
ASTM D2240
Tensile Strength 29.7 MPa
4310 psi
ASTM D412
Elongation at Break 690 %
690 %
ASTM D412
100% Modulus 0.00480 GPa
0.696 ksi
ASTM D412
300% Modulus 0.00660 GPa
0.957 ksi
ASTM D412
Tear Strength 17.9 kN/m
102 pli
Trouser; ASTM D470
Graves Tear Strength 59.6 kN/m
340 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 3.0
3.0
CS-17, 1000g; ASTM D3389 B
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -50.0 °C
-58.0 °F
DSC
Flammability, UL94 V-2
V-2
Processing Properties Metric English Comments
Zone 1 175 °C
347 °F
Extrusion
Zone 2 180 °C
356 °F
Extrusion
Zone 3 188 °C
370 °F
Extrusion
Zone 4 194 °C
381 °F
Extrusion
Adapter Temperature 194 °C
381 °F
Extrusion
Die Temperature 188 °C
370 °F
Zone 2, Extrusion
194 °C
381 °F
Zone 1, Extrusion
Drying Temperature 104 °C
219 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Dew Point -40.0 °C
-40.0 °F
Copyright © lookpolymers.com All Rights Reserved