Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 15.0 - 60.0 °C | 59.0 - 140 °F | |
SABIC MG200024 Linear Low Density Polyethylene for Compounding Product Description: MG200024 is a Linear Low Density Polyethylene grade with a narrow molecular weight distribution primarily suitable for compounding. It is in the powder form designed to give g.. |
|||
Mold Temperature | 15.0 - 40.0 °C | 59.0 - 104 °F | |
SABIC PP 412MK49 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 412MK49 is specially developed for producing injection molded articles. This grade contains an antistatic & nucleating agents. It has medium flow properties, good impact r.. |
|||
Mold Temperature | 15.0 - 40.0 °C | 59.0 - 104 °F | |
SABIC PP 49MK40 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 49MK40 is a high crystalline impact copolymer with high stiffness. This grade is especially developed for producing injection molded articles. The grade contains an antist.. |
|||
Mold Temperature | 15.0 - 40.0 °C | 59.0 - 104 °F | |
SABIC PP 49MK45 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 49MK45 is specially developed for producing injection molded articles. This grade contains an antistatic & nucleating agents. It has medium flow properties, good impact re.. |
|||
Mold Temperature | 15.0 - 40.0 °C | 59.0 - 104 °F | |
SABIC PP 513MN40 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 513MN40 is a controlled rheology PP grade of narrow molecular weight distribution. It contains an antistatic agent and is especially developed for producing injection molde.. |
|||
Mold Temperature | 15.0 - 40.0 °C | 59.0 - 104 °F | |
SABIC PP 5703P Polypropylene Homopolymer for Injection Molding Product Description: PP 5702P is specially developed for producing rigid injection molded articles for general purpose applications. It gives consistent processability and high gloss in the produc.. |
|||
Mold Temperature | 15.0 - 40.0 °C | 59.0 - 104 °F | |
SABIC PP 5707N Polypropylene Homopolymer STIFFPACT for Injection Molding Product Description: PP 5707N is a reactor PP homopolymer grade with antistatic and nucleated agents. It is suitable for producing injection molded applications and gives consistent processability.. |
|||
Mold Temperature | 15.0 - 40.0 °C | 59.0 - 104 °F | |
SABIC PP 575P Polypropylene Homopolymer for Injection Molding Product Description: PP 575P is specially developed for producing rigid injection molding articles for general purpose applications. It gives consistent processability and high gloss in the produc.. |
|||
Mold Temperature | 15.0 - 60.0 °C | 59.0 - 140 °F | |
SABIC M200056 High Density Polyethylene for Injection Molding Product Description: M200056 is a high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to provide good flow.. |
|||
Mold Temperature | 15.0 - 60.0 °C | 59.0 - 140 °F | |
SABIC M80064 Series High Density Polyethylene for Injection Molding Product Description: M80064 is a high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to provide good rigid.. |
|||
Mold Temperature | 15.0 - 80.0 °C | 59.0 - 176 °F | Average value: 49.8 °C Grade Count:71 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Mold Temperature | 15.0 - 50.0 °C | 59.0 - 122 °F | |
Inno-Comp INNOPOL® CS 2-3840 MO 40% Glass Filled Polypropylene Copolymer INNOPOL® CS 2-3840 MO is a 40 % glass-fiber-filled polypropylene block-copolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 2-3840 MO is recommended for p.. |
|||
Mold Temperature | 15.0 - 50.0 °C | 59.0 - 122 °F | |
Inno-Comp INNOPOL® CS 2-5830 SA 30% Glass Filled Polypropylene Copolymer INNOPOL® CS 2-5830 SA is a 30 % glass-fiber-filled polypropylene block-copolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 2-5830 SA is recommended for p.. |
|||
Mold Temperature | 15.0 - 50.0 °C | 59.0 - 122 °F | |
Inno-Comp INNOPOL® CS 3-8000 FR Flame Retardant Polypropylene Blend INNOPOL® CS 3-8000 FR is a flame retarded polypropylene compound based on a specific blend of polypropylene homo polymer and copolymer. This grade is available in natural and custom colored form... |
|||
Mold Temperature | 15.0 - 50.0 °C | 59.0 - 122 °F | |
Lotte Chemical Titan TITANLENE® LDI300YY Low density polyethylene resin LDI300YY is a low density polyethylene resin for injection molding and is a barefoot grade. LDI300YY meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 2.. |
|||
Mold Temperature | 15.0 - 50.0 °C | 59.0 - 122 °F | |
Inno-Comp INNOPOL® CS 1-2120 AP 20% Talc Filled Polypropylene Homopolymer INNOPOL CS 1-2120 AP is a 20 % talc filled compound based on polypropylene homopolymer. This grade is available in natural and custom colored form.INNOPOL® CS 1-2120 AP is recommended especially.. |
|||
Mold Temperature | 15.0 - 60.0 °C | 59.0 - 140 °F | |
Lubrizol Pellethane® 2363-80AE Thermoplastic Polyurethane Elastomer Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Mold Temperature | 15.0 - 40.0 °C | 59.0 - 104 °F | |
Borealis RG460MO Polypropylene, Transparent Random Copolymer RG460MO is a specially modified transparent polypropylene random copolymer with high melt flow. and is designed for high-speed injection molding and contains nucleating and demolding additives. Pro.. |
|||
Mold Temperature | 15.0 - 40.0 °C | 59.0 - 104 °F | |
Borealis RJ900MO Polypropylene Random Copolymer RJ900MO is a polypropylene random copolymer with high melt flow and good transparency. Products originating from this grade have excellent transparency and gloss, and good balance of stiffness and .. |
|||
Mold Temperature | 15.0 - 32.0 °C | 59.0 - 89.6 °F | Injection |
Lubrizol Estane® 58123 Thermoplastic Polyurethane Features: High moisture vapor transmission with low water swell and excellent low temperature and elasticity properties.Uses: Blown and flat die/cast film extrusion, injection molding and cable jack.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman DuraStar DS1110UVI Polymer, Natural Durastar DS1110UVI polymer, contains an ultraviolet light stabilization package. It is recommended for indoor applications requiring enhanced color stability upon extended exposure to fluorescent li.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman DuraStar DS2110UVI Polymer, Natural Durastar DS2110UVI polymer, contains an ultraviolet light stabilization package. It is recommended for indoor applications requiring enhanced color stability upon extended exposure to fluorescent li.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman DuraStar MN621 Polymer, Natural Durastar Polymer MN621 was developed for the medical device industry and contains a mold release It processes easily and requires minimal drying time. It has superior toughness, high clarity and goo.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman DuraStar MN630 Polymer, Natural Durastar Polymer MN630 has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. MN630 has very .. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman Eastar AN001 Copolyester, Natural Eastar AN001 Copolyester has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilities. Exposure to aromatic oils often ca.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman Eastar BR001 Copolyester Eastar BR001 Copolyester has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilities. Exposure to aromatic oils often ca.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman Eastar DN004HF Copolyester Applications:DisplaysPersonal care and CosmeticsProduct Description: Eastar Copolyester DN004HF has excellent flow characteristics while maintaining superior mechanical properties. It is easy to p.. |
|||
Mold Temperature | 15.0 - 50.0 °C | 59.0 - 122 °F | EBM |
Eastman Tritan TX1800 Copolyester Applications:Consumer and durable goodsExtrusion blow moldingInjection stretch blow moldingKey Attributes:Ease of processingExcellent clarityExcellent Hydrolytic stabilityGood chemical resistanceGoo.. |
|||
Mold Temperature | 15.0 - 50.0 °C | 59.0 - 122 °F | EBM Blow Mold Temp. |
Eastman Tritan WX500 Copolyester Eastman Tritan WX500 is a resin specifically developed for blow molded bottles. Extremely high melt strength makes the resin an excellent choice when manufacturing large bottles. This new-generati.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
LATI Latimass 37 B01-01 D025 Bio-Polymer Specific density compound based on Bio-Polymer (PLA, PHB, ...). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |