Material Notes:
Characteristicswide hardness rangedoes not require vulcanisation-quite higher saving on the processing costsremains flexible at low temperatureselectrical insulator with very low conductivityhas grades with very low conductivityhas grades with very low compression setgrades with very high abrasion resistanceexcellent tear resistance100% recyclablePVC freeresistance to acids, bases, and detergentsresistance to bacterial and fungus growthhas low toxic potential, with many grades conforming with FDA regulationshalogen free flame retardancycoloured grades availableallows direct colouring during processing by utilizing coloured PP and PE masterbatches2-shot moulding onto many other plasticsappropriate co-extrusion process
Physical Properties Metric English Comments
Density >= 0.890 g/cc
>= 0.0322 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
Hardness, Shore D 20
20
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 65.0 °C
149 °F
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Shrinkage 0.50 - 2.0 %
0.50 - 2.0 %
Processing Properties Metric English Comments
Rear Barrel Temperature 150 - 180 °C
302 - 356 °F
Middle Barrel Temperature 150 - 180 °C
302 - 356 °F
Front Barrel Temperature 150 - 180 °C
302 - 356 °F
Die Temperature 140 - 180 °C
284 - 356 °F
Mold Temperature 15.0 - 30.0 °C
59.0 - 86.0 °F
Descriptive Properties Value Comments
Acid-Base Resistance good
Comp. Ratio 1.5 - 3.0
Compression Set medium
Draw Down 5-10
Drying not necessary
Injection Speed fast
L/D Ratio 15 - 24:1
Motor Oil Resistance poor
Solvent Resistance poor
UV-Ozone Stability medium