Material Notes:
Eastar Polyester EN063 is a condensation polymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Eastar Polyester EN063 is a homopolymer PET that has been crystallized.Applications/UsesMedical
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 cm/cm

@Thickness 3.20 mm
0.0030 in/in

@Thickness 0.126 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 109
109
ASTM D785
Tensile Strength at Break 32.0 MPa
4640 psi
ASTM D638
Tensile Strength, Yield 58.0 MPa
8410 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Flexural Yield Strength 80.0 MPa
11600 psi
ASTM D790
Flexural Modulus 2.50 GPa
363 ksi
ASTM D790
Izod Impact, Notched 0.310 J/cm

@Temperature -40.0 °C
0.581 ft-lb/in

@Temperature -40.0 °F
ASTM D256
0.530 J/cm

@Temperature 23.0 °C
0.993 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D4812
20.0 J/cm

@Temperature -40.0 °C
37.5 ft-lb/in

@Temperature -40.0 °F
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 71.0 °C
160 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °C
147 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 275 - 295 °C
527 - 563 °F
Mold Temperature 10.0 - 30.0 °C
50.0 - 86.0 °F
Drying Temperature 150 - 160 °C
302 - 320 °F
Dry Time 4 - 6 hour
4 - 6 hour