Injection molding grade. Nylene 406 is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles through rapid melt set-up. Parts molded from 406 have better dimensional stability at moisture equilibrium than parts molded from conventional nylon.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 54.0 MPa
7830 psi
ASTM D638
Elongation at Break 250 %
250 %
ASTM D638
Izod Impact, Notched 2.50 J/cm
4.68 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 182 °C
360 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 232 - 243 °C
450 - 469 °F
At Nozzle
Nozzle Temperature 232 - 243 °C
450 - 469 °F