Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 204 - 232 °C | 399 - 450 °F | |
PolyOne Versaflex™ HC 2110-57B Thermoplastic Elastomer (TPE) Versaflex™ HC 2110-57B is a TPE designed for use in the healthcare industry offering low stiction and good compression set. New Product. Commercial specifications have not been established. - Bonds.. |
|||
Nozzle Temperature | 204 - 243 °C | 399 - 469 °F | |
PolyOne Versaflex™ OM 3060-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 3060-1 is a clear, medical compliant overmold designed to adhere to multiple substrates. - Excellent bond to PC, ABS, PC/ABS, PC/PETG, and PC/PBT - Rubber Feel - Soft TouchVersaflex™.. |