Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 232 - 243 °C | 450 - 469 °F | |
Nylene® 401, Nylon 6 Injection molding grade. Dry As Molded. Nylene 401 is recommended for general purpose nylon molding applications in both thin and heavy sections. Nylene 401 has high flow characteristics at minima.. |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 469 °F | |
Nylene® 401, Nylon 6, at 50% Relative Humidity Injection molding grade. Nylene 401 is recommended for general purpose nylon molding applications in both thin and heavy sections. Nylene 401 has high flow characteristics at minimal processing temp.. |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 469 °F | |
Nylene® 401D, Nylon 6 Injection molding grade. Dry as molded. Nylene 401D is a specially formulated nylon 6 molding resin possessing outstanding flow characteristics. Nylene 401D is ideally suited for applications requi.. |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 469 °F | |
Nylene® 402 Nylon 6 Injection molding grade. Dry as molded. Nylene 402 is a high monomer resin which offers outstanding toughness and flexibility. Nylene 402 exhibits excellent flow properties at temperature and press.. |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 469 °F | |
Nylene® 404 Nylon 6 Injection molding grade. Dry as molded. Nylene 404 is a heat stabilized version of 401 which is recommended for general purpose nylon molding applications in both thin and heavy sections. In additi.. |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 469 °F | |
Nylene® 404 Nylon 6, 50% RH Injection molding grade. Nylene 404 is a heat stabilized version of 401 which is recommended for general purpose nylon molding applications in both thin and heavy sections. In addition to protection.. |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 469 °F | |
Nylene® 406 Nylon 6 Injection molding grade. Dry as molded. Nylene 406 is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles through rapid melt set-up. Parts molded f.. |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 469 °F | |
Nylene® 406 Nylon 6, 50% RH Injection molding grade. Nylene 406 is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles through rapid melt set-up. Parts molded from 406 have bet.. |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 469 °F | |
Nylene® 406F Nylon 6 Dry as molded. Injection molding grade. Nylene 406F is a resin formulated to comply with FDA regulation 21 CFR 177.1500 for food contact applications. Nylene 406F is a general purpose, fast cycling.. |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 469 °F | |
Nylene® 406F Nylon 6, 50% RH Injection molding grade. Nylene 406F is a resin formulated to comply with FDA regulation 21 CFR 177.1500 for food contact applications. Nylene 406F is a general purpose, fast cycling molding resin.
.. |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 469 °F | |
Nylene® 409 Nylon 6 Dry as molded. Injection molding grade. Nylene 409 is a heat stabilized version of 406 which is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles.. |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 469 °F | |
Nylene® 409 Nylon 6, 50% RH Injection molding grade. Nylene 409 is a heat stabilized version of 406 which is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles through rapid m.. |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 469 °F | |
Nylene® 452 Nylon 6 Dry as molded. Injection molding grade. Nylene 452 is a plasticized, injection molding nylon for use in applications requiring high flexibility, and excellent toughness and abrasion resistance. Bec.. |
|||
Nozzle Temperature | 204 - 243 °C | 399 - 469 °F | |
PolyOne Versaflex™ OM 3060-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 3060-1 is a clear, medical compliant overmold designed to adhere to multiple substrates. - Excellent bond to PC, ABS, PC/ABS, PC/PETG, and PC/PBT - Rubber Feel - Soft TouchVersaflex™.. |
|||
Nozzle Temperature | 221 - 243 °C | 430 - 469 °F | Average value: 231 °C Grade Count:4 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum .. |