Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 180 - 190 °C | 356 - 374 °F | Plasticizing Zone |
Petroquimica Triunfo Trilene® TS 5009 LLDPE-C4 and LDPE Blend The Trilene TS 5009 product is a blend with a high ratio of linear low-density polyethylene (LLDPE) with low-density polyethylene (LDPE) with elevated processability, ensuring the production of film.. |
|||
Processing Temperature | 180 - 190 °C | 356 - 374 °F | Mixture Zone; Coextrusion with polyamide |
Petroquimica Triunfo Trithene® TN 7006 LDPE - Coextruded Film The Trithene® TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and streng.. |
|||
Processing Temperature | 180 - 190 °C | 356 - 374 °F | Mixture Zone; Coextrusion with polyamide |
Petroquimica Triunfo Trithene® TS 7006 LDPE - Coextruded Film The Trithene TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and strength.. |
|||
Processing Temperature | 160 - 190 °C | 320 - 374 °F | Sheet Forming |
Polycasa CAST PMMA QUINN CAST has an optical transparency of 93% light transmission for transparent sheets. It is significantly lighter and much more impact resistant than glass of equivalent thickness. QUINN CAST is .. |
|||
Processing Temperature | 180 - 190 °C | 356 - 374 °F | Plasticizing Zone |
Petroquimica Triunfo Trilene® TS 8058 LLDPE-C6 and LDPE Blend The Trilene TS 8058 product is a blend with a high ratio of linear low-density polyethylene - hexene comonomer (LLDPE-C6) with low-density polyethylene (LDPE) excellent mechanical resistance, along .. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | Molding temperature |
Cookson Group Plaskon® 3300SGH Mineral Filled Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.Exhibits exceptional reliability, excellent moldability, good release characteristics, low flash and rapid cure. This compound i.. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | Molding temperature |
Cookson Group Plaskon® 3300SH Mineral Filled Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.Exhibits exceptional reliability, excellent moldability, good release characteristics and low flash. This compound is especially.. |
|||
Processing Temperature | 160 - 190 °C | 320 - 374 °F | |
LG Chemical LUTENE BB0808 LDPE Blown Film Grade Description: LUTENE BB0808 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of shrink film and pallet shrink covers. LUTENE BB0808 have the balanc.. |
|||
Processing Temperature | 160 - 190 °C | 320 - 374 °F | Profiles and hoses |
Lucobit Lucofin® 1400MN Ethylene Butyl Acrylate Lucofin 1400MN is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400MN is softer and more flexible than ethylene homopoly.. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | |
Taiwan Sheen Soon Sheenthane® A7551E2 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Processing Temperature | 160 - 190 °C | 320 - 374 °F | |
Taiwan Sheen Soon Sheenthane® A8760 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Processing Temperature | 160 - 190 °C | 320 - 374 °F | |
Taiwan Sheen Soon Sheenthane® A8760F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Processing Temperature | 160 - 190 °C | 320 - 374 °F | |
Taiwan Sheen Soon Sheenthane® A8900F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | Metering Temperature, Extrusion |
Stellarchem GP-915UB TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | Metering Temperature, Extrusion |
Stellarchem GP-950 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | Metering Temperature, Extrusion |
Stellarchem GP-975B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | Metering Temperature, Extrusion |
Stellarchem MP-930HD TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Processing Temperature | 175 - 190 °C | 347 - 374 °F | |
Wanhua Chemical Wanthane® WHT-8280 Polyether-Based TPU Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | |
Wanhua Chemical Wanthane® WHT-A880 Aliphatic TPU Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Processing Temperature | 160 - 190 °C | 320 - 374 °F | |
Total EVA 1005 VN 2 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 2 is made by a high pressure tubular process. Grade for transparent and resistant films. Contains an antioxidant.Application examples: Stretch, coextrusion, frozen food, agriculture fi.. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | |
Wanhua Chemical Wanthane® WHT-1565 Polyester Based TPU Plasticizer free, excellent abrasion & slip resistance, low temperature flexibility, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Processing Temperature | 150 - 190 °C | 302 - 374 °F | Films Die Head |
EMS-Griltech Griltex® D 1439E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 150 - 190 °C | 302 - 374 °F | Films Die Head |
EMS-Griltech Griltex® D 1519E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 150 - 190 °C | 302 - 374 °F | Films Die Head |
EMS-Griltech Griltex® D 1556A Copolyamide Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 180 - 190 °C | 356 - 374 °F | |
Fainplast Compounds EVAtech 801S Ethylene Vinyl Acetate Foam EVA (ethylene-vinyl acetate) designed for the production of crosslinked expanded products using injection technology.Information provided by Fainplast Compounds |
|||
Processing Temperature | 180 - 190 °C | 356 - 374 °F | |
Fainplast Compounds EVAtech 803S Ethylene Vinyl Acetate Foam EVA (ethylene-vinyl acetate) designed for the production of crosslinked expanded products using injection technology.Information provided by Fainplast Compounds |
|||
Processing Temperature | 180 - 190 °C | 356 - 374 °F | |
Fainplast Compounds EVAtech 807I Ethylene Vinyl Acetate Foam EVA (ethylene-vinyl acetate) designed for the production of crosslinked expanded products using injection technology.Information provided by Fainplast Compounds |
|||
Processing Temperature | 150 - 190 °C | 302 - 374 °F | |
Total LDPE 1022 FN 24 Low Density Polyethylene - Blown Film LDPE 1022 FN 24 is a low density polyethylene made by a high pressure process without antioxidant.LDPE 1022 FN 24 is suited to many applications in the field of consumer, industrial, food or hygiene.. |
|||
Processing Temperature | 160 - 190 °C | 320 - 374 °F | Blown film |
Lucobit Lucofin® 1400HN Ethylene Butyl Acrylate Lucofin 1400HN is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400HN is softer and more flexible than ethylene homopolym.. |