Petroquimica Triunfo Trithene® TS 7006 LDPE - Coextruded Film

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Petroquimica Triunfo
Trade Name Trithene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Petroquimica Triunfo Trithene® TS 7006 LDPE - Coextruded Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Trithene TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and strength meet all the requirements for barrier films coextrusion, even for very thin structures. The antioxidant package allows for very good thermal stability during processing. This product complies with ASTM standard D1248-IA4 and the requirements of Brazilian and corresponding legislation of Mercosul and it is in conformity with FDA Regulations 21 CFR 177.1520 (c) 2.1, to contact with foodstuff.Applications: High clarity films, coextruded with polyamide, EVOH, PVdC, etc. for food packaging, such as: cheese, meat, sausages, sliced ham, etc.Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR.Information provided by Dax Resinas
Physical Properties Metric English Comments
Density 0.923 - 0.926 g/cc
0.0333 - 0.0335 lb/in³
ASTM D1505
Thickness 50.0 microns
1.97 mil
Melt Index of Compound 0.50 - 0.70 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.50 - 0.70 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 16.0 MPa
2320 psi
ASTM D638
Tensile Strength, Yield 12.0 MPa
1740 psi
ASTM D638
Film Elongation at Break, MD 350 %
350 %
ASTM D882
Film Elongation at Break, TD 700 %
700 %
ASTM D882
Elongation at Break 575 %
575 %
ASTM D638
Secant Modulus, MD 0.117 GPa
17.0 ksi
5%; ASTM D882
Secant Modulus, TD 0.125 GPa
18.1 ksi
5%; ASTM D882
Coefficient of Friction, Dynamic 0.15
0.15
ASTM D1894
Elmendorf Tear Strength, MD 7.40 g/micron
188 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 5.70 g/micron
145 g/mil
ASTM D1922
Dart Drop Test 160 g
0.353 lb
(method A); ASTM D1709
Film Tensile Strength at Break, MD 26.0 MPa
3770 psi
ASTM D882
Film Tensile Strength at Break, TD 23.0 MPa
3340 psi
ASTM D882
Thermal Properties Metric English Comments
Vicat Softening Point 97.0 °C
207 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 9.0 %
9.0 %
ASTM D1003
Gloss 85 %
85 %
@ 60° Gardner; ASTM D2457
Processing Properties Metric English Comments
Processing Temperature 155 - 165 °C
311 - 329 °F
Plasticizing Zone; Monoextrusion
165 - 175 °C
329 - 347 °F
Mixture Zone; Monoextrusion
170 - 180 °C
338 - 356 °F
Plasticizing Zone; Coextrusion with polyamide
180 - 190 °C
356 - 374 °F
Mixture Zone; Coextrusion with polyamide
Feed Temperature 150 - 160 °C
302 - 320 °F
Mono-extrusion
160 - 170 °C
320 - 338 °F
Co-extrusion with Polyamide
Adapter Temperature 175 - 185 °C
347 - 365 °F
Mono-extrusion
220 - 230 °C
428 - 446 °F
Co-extrusion with Polyamide
Blow-up Ratio (BUR) 3.0
3.0
Recommended