Material Notes:
Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ASTM D2240
Tensile Strength 14.0 MPa
2030 psi
ASTM D412
Elongation at Break 550 %
550 %
ASTM D412
100% Modulus 0.00400 GPa
0.580 ksi
ASTM D412
300% Modulus 0.00700 GPa
1.02 ksi
ASTM D412
Tear Strength 55.0 kN/m
314 pli
ASTM D624
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -55.0 °C
-67.0 °F
Processing Properties Metric English Comments
Processing Temperature 170 - 190 °C
338 - 374 °F