Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.150 W/m-K | 1.04 BTU-in/hr-ft²-°F | |
Quadrant EPP Symalit® 1000 ECTFE, unfilled, lining industries (ISO Data) Symalit 1000 ECTFE is made from a fluoropolymer resin that is a copolymer of ethylene and chlorotrifluoroethylene. It exhibits good mechanical properties combined with an excellent chemical resistan.. |
|||
Thermal Conductivity | 0.150 W/m-K | 1.04 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® FL900 PC (Asia Pacific) Various weight reductions at 0.250"" (6.35 mm). High heat/creep resistance excellent impact, flexural strength/rigidity. UL94 V-1 at .157"" (3.99 mm). |
|||
Thermal Conductivity | 0.150 W/m-K | 1.04 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Lexan® FL900P PC (Europe-Africa-Middle East) Foamable LEXAN, various weight reductions at 6.4 mm. Offers load bearing capability at elavated temp., Combines rigidity, impact & toughness.This data was supplied by SABIC-IP for the Europe-Africa-.. |
|||
Thermal Conductivity | 0.150 W/m-K | 1.04 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Lexan® FL900S PC (Europe-Africa-Middle East) Foamable Lexan* FL900S polycarbonate resin is an ideal choice for structural components where load bearing capability at elevated temperature is a key requirement. It exhibits outstanding inpact str.. |
|||
Thermal Conductivity | 0.150 W/m-K @Temperature 40.0 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
Solvay Specialty Polymers Halar® 1450LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**) Information provided by Solvay Specialty Polymers. |
|||
Thermal Conductivity | 0.150 W/m-K @Temperature 40.0 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
Solvay Specialty Polymers Halar® 300DA Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Halar® "DA" grades are available and meet the FDA's Condition of Use B, as described under 21 C.F.R. 176-170(c).Information provided by Solvay Specialty Polymers. |
|||
Thermal Conductivity | 0.150 W/m-K @Temperature 40.0 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
Solvay Specialty Polymers Halar® 350LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Thermal Conductivity | 0.150 W/m-K @Temperature 40.0 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
Solvay Specialty Polymers Halar® 5001C Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Powder grades for masterbatches.Information provided by Solvay Specialty Polymers. |
|||
Thermal Conductivity | 0.150 W/m-K @Temperature 40.0 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
Solvay Specialty Polymers Halar® 500LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Thermal Conductivity | 0.150 W/m-K @Temperature 40.0 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
Solvay Specialty Polymers Halar® 902 Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)< Information provided by Solvay Specialty Polymers. |
|||
Thermal Conductivity | 0.150 - 0.251 W/m-K | 1.04 - 1.74 BTU-in/hr-ft²-°F | Average value: 0.238 W/m-K Grade Count:11 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |
|||
Thermal Conductivity | 0.150 - 0.216 W/m-K | 1.04 - 1.50 BTU-in/hr-ft²-°F | Average value: 0.179 W/m-K Grade Count:3 |
Overview of materials for Fluorocarbon ETFE/ECTFE, Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE/ECTFE, Molded/Extruded". Each property range of values reported is minimum and maximum.. |
|||
Thermal Conductivity | 0.150 - 0.150 W/m-K @Temperature 40.0 - 40.0 °C |
1.04 - 1.04 BTU-in/hr-ft²-°F @Temperature 104 - 104 °F |
Average value: 0.150 W/m-K Grade Count:13 |
Overview of materials for ECTFE Fluoropolymer This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Thermal Conductivity | 0.150 W/m-K | 1.04 BTU-in/hr-ft²-°F | DIN 52612 |
Isoflon ECTFE Fluoropolymer Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Thermal Conductivity | 0.150 W/m-K | 1.04 BTU-in/hr-ft²-°F | |
Isoflon Polyester film Polyethylene terephthalate film is a flexible film with high mechanical resistance. An excellent insulator, it preserves all its properties in a wide range of temperatures (-70°C to +150°C). .. |
|||
Thermal Conductivity | 0.150 W/m-K @Temperature 40.0 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
Solvay Specialty Polymers Ajedium™ Films -- Halar® 500LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Halar® ECTFE is a semi-crystalline fluoropolymer with a chemical structure of a 1:1 alternating copolymer of ethylene and chlorotrifluoroethylene.Halar® film is a strong, hard, tough, abrasion.. |
|||
Thermal Conductivity | 0.150 W/m-K @Temperature 40.0 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
Solvay Specialty Polymers Halar® 1400LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: FibersAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 300 °CInformation provided by Solvay Spec.. |
|||
Thermal Conductivity | 0.150 W/m-K @Temperature 40.0 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
Solvay Specialty Polymers Halar® 350LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol.. |
|||
Thermal Conductivity | 0.150 W/m-K @Temperature 40.0 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
Solvay Specialty Polymers Halar® 5001C Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Powder grades for masterbatches.Features: Low ViscosityUses: Masterbatch; Wire & Cable ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0.. |
|||
Thermal Conductivity | 0.150 W/m-K @Temperature 40.0 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
Solvay Specialty Polymers Halar® 513LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: MonofilamentsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solv.. |
|||
Thermal Conductivity | 0.150 W/m-K @Temperature 40.0 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
Solvay Specialty Polymers Halar® 930LCW Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol.. |
|||
Thermal Conductivity | 0.150 W/m-K | 1.04 BTU-in/hr-ft²-°F | |
Shin-Etsu Silicones KE-109A/B Silicone, Potting/Encapsulation RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Thermal Conductivity | 0.150 W/m-K @Temperature 1600 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 2910 °F |
|
Sinotek Materials Rigid Graphite Felt Board Heat Insulation Material Information provided by Sinotek |
|||
Thermal Conductivity | 0.150 W/m-K @Temperature 40.0 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
Solvay Specialty Polymers Halar® 901 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) High ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polym.. |
|||
Thermal Conductivity | 0.150 W/m-K @Temperature 40.0 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
Solvay Specialty Polymers Halar® 902 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) High ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 28.0 J/g; Heat of Fusion - ASTM D3418 28.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polym.. |
|||
Thermal Conductivity | 0.150 W/m-K | 1.04 BTU-in/hr-ft²-°F | |
Goodfellow Polyhydroxybutyrate / Polyhydroxyvalerate (PHB 92/PHV 8) See also PHB. PHB/PHV copolymers are used in preference to PHB homopolymer for general purposes (e.g. molding containers) in order to obtain a better balance of stiffness and toughness. PHV contents.. |
|||
Thermal Conductivity | 0.150 W/m-K | 1.04 BTU-in/hr-ft²-°F | |
Goodfellow Polyhydroxybutyrate/Polyhydroxyvalerate (PHB 88/PHV 12) See also PHB. PHB/PHV copolymers are used in preference to PHB homopolymer for general purposes (e.g. molding containers) in order to obtain a better balance of stiffness and toughness. PHV contents.. |
|||
Thermal Conductivity | 0.151 W/m-K | 1.04 BTU-in/hr-ft²-°F | |
Dow VORANOL™ 4240 Polyether Polyol VORANOL™ 4240 polyether polyol is a nominal 4000 molecular weight diol based on propylene oxide with ethylene oxide capping. Its high molecular weight and enhanced reactivity make it well suited t.. |