Polikim EFALON® T-100 Virgin PTFE

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Polikim Polimer ve Kimya Sanay
Trade Name EFALON®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polikim EFALON® T-100 Virgin PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Gaskets, seals, O-rings, V-Rings, compression packings and similar sealing parts, Bushes, bearings and piston rings, Electrical insulators, Sliding supports, Conveyor belts, Coated tubes, valves and joint components for transfer of corrosive material, Non-stick surface applications, PTFE coated glass fabric manufacturing, Laboratory equipment that requires chemical resistance. In military units and marine industry due to resistance to water, humidity, micro-organisms and sunlight.Information provided by Polikim Polimer.
Physical Properties Metric English Comments
Density 2.10 - 2.20 g/cc
0.0759 - 0.0795 lb/in³
ASTM D792
Deformation 7.5 - 8.5 %

@Temperature 23.0 °C,
Time 86400 sec,
Pressure 13.7 MPa
7.5 - 8.5 %

@Temperature 73.4 °F,
Time 24.0 hour,
Pressure 1990 psi
permanent; ASTM D621
14 - 16.8 %

@Temperature 23.0 °C,
Time 86400 sec,
Pressure 13.7 MPa
14 - 16.8 %

@Temperature 73.4 °F,
Time 24.0 hour,
Pressure 1990 psi
total; ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 54 - 60
54 - 60
ASTM D2240
Tensile Strength, Ultimate 13.7 - 37.3 MPa
1990 - 5400 psi
ASTM D638
Elongation at Break 200 - 400 %
200 - 400 %
ASTM D638
Compressive Strength 4.41 - 4.90 MPa
640 - 711 psi
1% Deformation; ASTM D695
Izod Impact, Notched (ISO) 15.5 - 16.5 kJ/m²
7.38 - 7.85 ft-lb/in²
ASTM D256
Coefficient of Friction 0.060
0.060
Coefficient of Friction, Static 0.040
0.040
Limiting Pressure Velocity 0.000376 - 0.000409 MPa-m/sec
10.7 - 11.7 psi-ft/min
3 m/min
0.000605 - 0.000654 MPa-m/sec
17.3 - 18.7 psi-ft/min
30 m/min
0.0008502 - 0.0009156 MPa-m/sec
24.27 - 26.14 psi-ft/min
300 m/min
Thermal Properties Metric English Comments
CTE, linear 125 - 160 µm/m-°C

@Temperature 25.0 - 100 °C
69.4 - 88.9 µin/in-°F

@Temperature 77.0 - 212 °F
ASTM D696
150 - 190 µm/m-°C

@Temperature 25.0 - 200 °C
83.3 - 106 µin/in-°F

@Temperature 77.0 - 392 °F
ASTM D696
215 - 250 µm/m-°C

@Temperature 25.0 - 300 °C
119 - 139 µin/in-°F

@Temperature 77.0 - 572 °F
ASTM D696
Specific Heat Capacity 0.962 - 1.05 J/g-°C
0.230 - 0.251 BTU/lb-°F
Thermal Conductivity 0.230 - 0.251 W/m-K
1.59 - 1.74 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 270 °C
518 °F
continuous
Minimum Service Temperature, Air -260 °C
-436 °F
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+18 ohm-cm
>= 1.00e+18 ohm-cm
ASTM D257
Surface Resistance >= 1.00e+16 ohm
>= 1.00e+16 ohm
50% rel. humidity; ASTM D257
Dielectric Constant 2.0 - 2.1

@Frequency 50.0 - 1.00e+7 Hz
2.0 - 2.1

@Frequency 50.0 - 1.00e+7 Hz
ASTM D150
Dielectric Strength 40.0 - 80.0 kV/mm

@Thickness 0.100 mm
1020 - 2030 kV/in

@Thickness 0.00394 in
short term; ASTM D149
Dielectric Loss Index 0.000050

@Frequency 50.0 Hz
0.000050

@Frequency 50.0 Hz
dry