Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.150 W/m-K | 1.04 BTU-in/hr-ft²-°F | DIN.52612 |
Omnia Plastica PVC Polyvinylchloride A widely used material, its application is under regulation in many countries for ecological reasons and it is often substituted by PP or other polymers. It is chosen for its chemical resistance.Fea.. |
|||
Thermal Conductivity | 0.150 W/m-K | 1.04 BTU-in/hr-ft²-°F | |
Pyrotek LUMIFELT AL20 High Temperature Kevlar® Felt Lumifelt is composed of heat resistant para linked type Kevlar® fiber. Lumifelt is an ideal insulating pad for a variety of applications. It is needle punched to give it high tensile strength and.. |
|||
Thermal Conductivity | 0.150 W/m-K | 1.04 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® FL900 PC (Asia Pacific) Various weight reductions at 0.250"" (6.35 mm). High heat/creep resistance excellent impact, flexural strength/rigidity. UL94 V-1 at .157"" (3.99 mm). |
|||
Thermal Conductivity | 0.150 W/m-K | 1.04 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® FL900 PC Lexan* resin FL900 is a Br- & Cl-free flame retardant grade that can be foamed for weight reductions. UL-94 V1 listed at 3.9mm together with good stiffness, heat, creep and impact performance make i.. |
|||
Thermal Conductivity | 0.150 - 0.200 W/m-K | 1.04 - 1.39 BTU-in/hr-ft²-°F | Average value: 0.172 W/m-K Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Thermal Conductivity | 0.150 W/m-K | 1.04 BTU-in/hr-ft²-°F | ASTM C177 |
Covestro Makrolon® SF-800 Polycarbonate, Structural Foam
(discontinued **) Properties based on foam density of 0.90 g/cc.Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially.. |
|||
Thermal Conductivity | 0.150 W/m-K @Temperature 40.0 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
Solvay Specialty Polymers Halar® 1450LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**) Information provided by Solvay Specialty Polymers. |
|||
Thermal Conductivity | 0.150 W/m-K @Temperature 40.0 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
Solvay Specialty Polymers Halar® 300LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(discontinued **) Information provided by Solvay Specialty Polymers. |
|||
Thermal Conductivity | 0.150 W/m-K @Temperature 40.0 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
Solvay Specialty Polymers Halar® 350LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Thermal Conductivity | 0.150 W/m-K @Temperature 40.0 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
Solvay Specialty Polymers Halar® 500LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Thermal Conductivity | 0.150 W/m-K @Temperature 40.0 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
Solvay Specialty Polymers Halar® 513LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Thermal Conductivity | 0.150 - 0.251 W/m-K | 1.04 - 1.74 BTU-in/hr-ft²-°F | Average value: 0.238 W/m-K Grade Count:11 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |
|||
Thermal Conductivity | 0.150 - 0.216 W/m-K | 1.04 - 1.50 BTU-in/hr-ft²-°F | Average value: 0.179 W/m-K Grade Count:3 |
Overview of materials for Fluorocarbon ETFE/ECTFE, Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE/ECTFE, Molded/Extruded". Each property range of values reported is minimum and maximum.. |
|||
Thermal Conductivity | 0.150 - 0.150 W/m-K @Temperature 40.0 - 40.0 °C |
1.04 - 1.04 BTU-in/hr-ft²-°F @Temperature 104 - 104 °F |
Average value: 0.150 W/m-K Grade Count:13 |
Overview of materials for ECTFE Fluoropolymer This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Thermal Conductivity | 0.150 W/m-K | 1.04 BTU-in/hr-ft²-°F | |
Natural Rubber, Vulcanized (NR, IR, Polyisoprene) Natural rubber is polyisoprene. Chemical and environmental resistance and mechanical properties are improved through crosslinking (vulcanizing), usually through treatment with sulfur.Natural rubber.. |
|||
Thermal Conductivity | 0.150 W/m-K | 1.04 BTU-in/hr-ft²-°F | DIN 52612 |
GEHR Plastics ECTFE Polyethylene Chlorotrifluoroethylene Ethylene-Chlortrifluorethylene exhibits an extraordinary impact strength at temperatures ranging from -76°C to 150°C. A great part of the product properties attributes to the very smooth surfa.. |
|||
Thermal Conductivity | 0.150 W/m-K | 1.04 BTU-in/hr-ft²-°F | DIN 52612 |
Isoflon ECTFE Fluoropolymer Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Thermal Conductivity | 0.150 W/m-K | 1.04 BTU-in/hr-ft²-°F | |
Isoflon Polyester film Polyethylene terephthalate film is a flexible film with high mechanical resistance. An excellent insulator, it preserves all its properties in a wide range of temperatures (-70°C to +150°C). .. |
|||
Thermal Conductivity | 0.150 W/m-K @Temperature 40.0 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
Solvay Specialty Polymers Ajedium™ Films -- Halar® 500LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Halar® ECTFE is a semi-crystalline fluoropolymer with a chemical structure of a 1:1 alternating copolymer of ethylene and chlorotrifluoroethylene.Halar® film is a strong, hard, tough, abrasion.. |
|||
Thermal Conductivity | 0.150 W/m-K @Temperature 40.0 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
Solvay Specialty Polymers Halar® 1400LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: FibersAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 300 °CInformation provided by Solvay Spec.. |
|||
Thermal Conductivity | 0.150 W/m-K @Temperature 40.0 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
Solvay Specialty Polymers Halar® 300DA Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Halar® "DA" grades are available and meet the FDA's Condition of Use B, as described under 21 C.F.R. 176-170(c).Features: Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 .. |
|||
Thermal Conductivity | 0.150 W/m-K @Temperature 40.0 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
Solvay Specialty Polymers Halar® 350LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol.. |
|||
Thermal Conductivity | 0.150 W/m-K @Temperature 40.0 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
Solvay Specialty Polymers Halar® 930LCW Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol.. |
|||
Thermal Conductivity | 0.150 - 0.250 W/m-K @Temperature 40.0 °C |
1.04 - 1.74 BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
Solvay Specialty Polymers Hyflon® PFA 125 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Thermal Conductivity | 0.150 W/m-K @Temperature 1600 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 2910 °F |
|
Sinotek Materials Rigid Graphite Felt Board Heat Insulation Material Information provided by Sinotek |
|||
Thermal Conductivity | 0.150 W/m-K | 1.04 BTU-in/hr-ft²-°F | |
Goodfellow Polyhydroxybutyrate / Polyhydroxyvalerate (PHB 92/PHV 8) See also PHB. PHB/PHV copolymers are used in preference to PHB homopolymer for general purposes (e.g. molding containers) in order to obtain a better balance of stiffness and toughness. PHV contents.. |
|||
Thermal Conductivity | 0.150 W/m-K | 1.04 BTU-in/hr-ft²-°F | |
Goodfellow Polyhydroxybutyrate/Polyhydroxyvalerate (PHB 88/PHV 12) See also PHB. PHB/PHV copolymers are used in preference to PHB homopolymer for general purposes (e.g. molding containers) in order to obtain a better balance of stiffness and toughness. PHV contents.. |
|||
Thermal Conductivity | 0.150 W/m-K | 1.04 BTU-in/hr-ft²-°F | of melt |
DuPont Performance Polymers Hytrel® 6646 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 66 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |