Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded

Category Polymer , Thermoplastic , Fluoropolymer , FEP , Fluorinated Ethylene Propylene (FEP), Molded/Extruded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Fluorinated Ethylene Propylene (FEP), Molded/Extruded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.30 - 2.17 g/cc
0.0470 - 0.0784 lb/in³
Average value: 1.94 g/cc Grade Count:15
Water Absorption 0.00400 - 0.0300 %
0.00400 - 0.0300 %
Average value: 0.0113 % Grade Count:11
Oxygen Transmission 320 cc-mm/m²-24hr-atm
812 cc-mil/100 in²-24hr-atm
Average value: 320 cc-mm/m²-24hr-atm Grade Count:25
Nitrogen Transmission 104 cc-mm/m²-24hr-atm
263 cc-mil/100 in²-24hr-atm
Average value: 104 cc-mm/m²-24hr-atm Grade Count:25
Viscosity 0.0100 - 8.00 cP
0.0100 - 8.00 cP
Average value: 4.10 cP Grade Count:4
4.00e+6 - 4.00e+7 cP

@Temperature 380 - 380 °C
4.00e+6 - 4.00e+7 cP

@Temperature 716 - 716 °F
Average value: 2.20e+7 cP Grade Count:8
Thickness 12.7 - 5000 microns
0.500 - 197 mil
Average value: 1040 microns Grade Count:13
Linear Mold Shrinkage 0.0300 - 0.0600 cm/cm
0.0300 - 0.0600 in/in
Average value: 0.0450 cm/cm Grade Count:8
Melt Flow 0.800 - 37.0 g/10 min
0.800 - 37.0 g/10 min
Average value: 10.6 g/10 min Grade Count:8
Mechanical Properties Metric English Comments
Hardness, Shore D 55.0 - 65.0
55.0 - 65.0
Average value: 55.7 Grade Count:11
Tensile Strength, Ultimate 18.0 - 34.0 MPa
2610 - 4930 psi
Average value: 21.5 MPa Grade Count:11
Elongation at Break 245 - 400 %
245 - 400 %
Average value: 295 % Grade Count:11
Modulus of Elasticity 0.343 - 0.700 GPa
49.7 - 102 ksi
Average value: 0.378 GPa Grade Count:11
Flexural Modulus 0.539 - 0.655 GPa
78.2 - 95.0 ksi
Average value: 0.596 GPa Grade Count:10
Compressive Yield Strength 5.00 - 15.2 MPa
725 - 2200 psi
Average value: 6.57 MPa Grade Count:9
Izod Impact, Unnotched NB
NB
Grade Count:8
Coefficient of Friction 0.0400 - 0.350
0.0400 - 0.350
Average value: 0.0695 Grade Count:19
Coefficient of Friction, Static 0.0500
0.0500
Average value: 0.0500 Grade Count:8
Taber Abrasion, mg/1000 Cycles 6.00 - 24.0
6.00 - 24.0
Average value: 21.8 Grade Count:8
Thermal Properties Metric English Comments
CTE, linear 83.0 - 135 µm/m-°C
46.1 - 75.0 µin/in-°F
Average value: 98.9 µm/m-°C Grade Count:10
Thermal Conductivity 0.190 - 0.250 W/m-K
1.32 - 1.74 BTU-in/hr-ft²-°F
Average value: 0.238 W/m-K Grade Count:11
Melting Point 245 - 275 °C
473 - 527 °F
Average value: 264 °C Grade Count:10
Maximum Service Temperature, Air 200 - 205 °C
392 - 401 °F
Average value: 201 °C Grade Count:11
Flammability, UL94 V-0
V-0
Grade Count:26
Oxygen Index 95.0 %
95.0 %
Average value: 95.0 % Grade Count:27
Optical Properties Metric English Comments
Transmission, Visible 92.0 - 95.0 %
92.0 - 95.0 %
Average value: 93.5 % Grade Count:9
IR Transmittance 95.0 - 98.0 %
95.0 - 98.0 %
Average value: 96.5 % Grade Count:9
UV Transmittance 91.0 - 92.0 %
91.0 - 92.0 %
Average value: 91.5 % Grade Count:9
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+17 - 1.00e+18 ohm-cm
1.00e+17 - 1.00e+18 ohm-cm
Average value: 9.55e+17 ohm-cm Grade Count:10
Dielectric Constant 2.00 - 2.20
2.00 - 2.20
Average value: 2.10 Grade Count:27
Dielectric Strength 19.7 - 80.0 kV/mm
500 - 2030 kV/in
Average value: 33.5 kV/mm Grade Count:11
Dissipation Factor 0.0000600 - 0.000800
0.0000600 - 0.000800
Average value: 0.000251 Grade Count:26
Users viewing this material also viewed the following: