Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.230 - 0.251 W/m-K | 1.59 - 1.74 BTU-in/hr-ft²-°F | |
Polikim EFALON® T-100 Virgin PTFE Applications: Gaskets, seals, O-rings, V-Rings, compression packings and similar sealing parts, Bushes, bearings and piston rings, Electrical insulators, Sliding supports, Conveyor belts, Coated tu.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.59 BTU-in/hr-ft²-°F | |
Honeywell ACLAR® 22C (2.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |