Westlake Plastics Zelux® 10% GF Polycarbonate 10% Glass Filled

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 10% Glass Filled
Manufacturer Westlake Plastics
Trade Name Zelux®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Zelux® 10% GF Polycarbonate 10% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and impact strength are essential including lenses, manifolds, site glasses and machine guards. Zelux is used for a wide range of electrical applications since it has low moisture absorption and good insulating properties. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Water Absorption 0.12 %
0.12 %
ASTM D570; 24 hrs.
Water Absorption at Saturation 0.31 %
0.31 %
ASTM D570; at equilibrium
Mechanical Properties Metric English Comments
Hardness, Rockwell M 85
85
ASTM D7852
Hardness, Rockwell R 124
124
ASTM D7852
Tensile Strength at Break 55.2 MPa
8000 psi
ASTM D638
Tensile Strength, Yield 66.2 MPa
9600 psi
ASTM D638
Elongation at Break 15 %
15 %
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Tensile Modulus 3.10 GPa
450 ksi
ASTM D638
Flexural Yield Strength 103 MPa
15000 psi
ASTM D790
Flexural Modulus 3.45 GPa
500 ksi
ASTM D790
Compressive Strength 96.5 MPa
14000 psi
ASTM D695
Compressive Modulus 3.59 GPa
520 ksi
ASTM D695
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Izod Impact, Unnotched 21.4 J/cm
40.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 32.4 µm/m-°C

@Temperature 20.0 °C
18.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.200 W/m-K
1.39 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 146 °C
295 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 142 °C
288 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.47 mm
V-0

@Thickness 0.0580 in
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
ASTM D257
Dielectric Constant 3.1

@Frequency 60 Hz
3.1

@Frequency 60 Hz
ASTM D150
Dielectric Strength 45.0 kV/mm
1140 kV/in
ASTM D149
Dissipation Factor 0.00080

@Frequency 60 Hz
0.00080

@Frequency 60 Hz
ASTM D150