Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CMT Materials REN Shape® 5008 Vacuum Forming Tooling Board

Category Polymer
Manufacturer CMT Materials
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMT Materials REN Shape® 5008 Vacuum Forming Tooling Board.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
REN SHAPE 5008 is a tooling board specifically designed for use in vacuum forming. It is designed for use up to 250°F and is well suited for building vacuum forming molds as well as master models, lay-up tools for prepreg curing, and other heat resistant tooling. This moderate density epoxy system features a low coefficient of thermal expansion for outstanding accuracy and dimensional stability. REN SHAPE 5008 also offers the following:Good MachinabilitySuperior Edge Definition and Dimensional StabilityOutstanding Surface FinishApplications: REN SHAPE 5008 applications may include prototype and production vacuum forming molds, temporary intermediate-temperature master and lay-up tools and master models for composite parts.Information Provided by CMT Materials, Inc.
Physical Properties Metric English Comments
Density 0.673 g/cc
0.0243 lb/in³
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 68
68
ASTM D-2240
Tensile Strength, Ultimate 24.1 MPa
3500 psi
ASTM D-638
Flexural Strength 31.7 MPa
4600 psi
ASTM D-790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D-790
Compressive Strength 56.5 MPa
8200 psi
ASTM D-695
Compressive Modulus 2.41 GPa
350 ksi
ASTM D-695
Thermal Properties Metric English Comments
CTE, linear 32.4 µm/m-°C

@Temperature -30.0 - 30.0 °C
18.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D-3386
Glass Transition Temp, Tg 142 °C
287 °F
ASTM D-4065
Descriptive Properties Value Comments
Color Light Blue
Copyright © lookpolymers.com All Rights Reserved