Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PlastxWorld CEVIAN® S5230 30% GF PC/ABS alloy

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Glass Fiber Filled , Polycarbonate (PC)
Manufacturer PlastxWorld, Inc.
Trade Name CEVIAN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastxWorld CEVIAN® S5230 30% GF PC/ABS alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass fiber reinforced and flame retarded PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 125 MPa
18200 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Yield Strength 159 MPa
23000 psi
ASTM D790
Flexural Modulus 8.14 GPa
1180 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm

@Thickness 6.35 mm
1.50 ft-lb/in

@Thickness 0.250 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 32.4 µm/m-°C

@Temperature 20.0 °C
18.0 µin/in-°F

@Temperature 68.0 °F
ASTM D1525
Deflection Temperature at 1.8 MPa (264 psi) 137 °C
279 °F
0.25 inch; ASTM D648
Flammability, UL94 V-0

@Thickness 1.65 mm
V-0

@Thickness 0.0650 in
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved