This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.16 - 1.73 g/cc
0.0419 - 0.0625 lb/in³
Average value: 1.38 g/cc Grade Count:70
Filler Content 5.00 - 20.0 %
5.00 - 20.0 %
Average value: 10.2 % Grade Count:29
Water Absorption 0.100 - 0.300 %
0.100 - 0.300 %
Average value: 0.134 % Grade Count:34
Additive Loading 5.00 - 10.0 %
5.00 - 10.0 %
Average value: 8.14 % Grade Count:7
Linear Mold Shrinkage 0.00100 - 0.00750 cm/cm
0.00100 - 0.00750 in/in
Average value: 0.00434 cm/cm Grade Count:69
Linear Mold Shrinkage, Transverse 0.00400 - 0.00800 cm/cm
0.00400 - 0.00800 in/in
Average value: 0.00695 cm/cm Grade Count:5
Mechanical Properties Metric English Comments
Hardness, Rockwell R 124
124
Average value: 124 Grade Count:3
Tensile Strength, Ultimate 29.0 - 138 MPa
4210 - 20000 psi
Average value: 72.7 MPa Grade Count:55
Tensile Strength, Yield 29.0 - 90.3 MPa
4210 - 13100 psi
Average value: 64.1 MPa Grade Count:18
Elongation at Break 1.00 - 15.0 %
1.00 - 15.0 %
Average value: 5.41 % Grade Count:69
Elongation at Yield 1.80 - 4.80 %
1.80 - 4.80 %
Average value: 3.63 % Grade Count:3
Modulus of Elasticity 2.21 - 10.3 GPa
321 - 1490 ksi
Average value: 4.47 GPa Grade Count:50
Flexural Yield Strength 55.2 - 200 MPa
8010 - 29000 psi
Average value: 112 MPa Grade Count:68
Flexural Modulus 2.41 - 10.3 GPa
350 - 1490 ksi
Average value: 3.87 GPa Grade Count:65
Izod Impact, Notched 0.267 - 2.14 J/cm
0.500 - 4.01 ft-lb/in
Average value: 0.801 J/cm Grade Count:67
Izod Impact, Unnotched 2.08 - 5340 J/cm
3.90 - 10000 ft-lb/in
Average value: 7.33 J/cm Grade Count:55
Izod Impact, Notched (ISO) 4.90 - 11.0 kJ/m²
2.33 - 5.23 ft-lb/in²
Average value: 8.03 kJ/m² Grade Count:3
Izod Impact, Unnotched (ISO) 14.3 - 131 kJ/m²
6.80 - 62.3 ft-lb/in²
Average value: 76.8 kJ/m² Grade Count:3
Thermal Properties Metric English Comments
CTE, linear 32.4 - 68.0 µm/m-°C
18.0 - 37.8 µin/in-°F
Average value: 53.8 µm/m-°C Grade Count:11
Deflection Temperature at 0.46 MPa (66 psi) 91.1 - 146 °C
196 - 295 °F
Average value: 137 °C Grade Count:16
Deflection Temperature at 1.8 MPa (264 psi) 51.7 - 143 °C
125 - 290 °F
Average value: 132 °C Grade Count:45
Flammability, UL94 HB - V-0
HB - V-0
Grade Count:51
Electrical Properties Metric English Comments
Electrical Resistivity 0.100 - 1.00e+12 ohm-cm
0.100 - 1.00e+12 ohm-cm
Average value: 1.58e+10 ohm-cm Grade Count:64
Surface Resistance 0.100 - 1.00e+12 ohm
0.100 - 1.00e+12 ohm
Average value: 1.30e+10 ohm Grade Count:69
Static Decay 0.100 - 2.00 sec
0.100 - 2.00 sec
Average value: 1.48 sec Grade Count:51
Shielding Effectiveness 40.0 - 55.0 dB
40.0 - 55.0 dB
Average value: 50.4 dB Grade Count:13
Processing Properties Metric English Comments
Processing Temperature 266 - 293 °C
510 - 560 °F
Average value: 279 °C Grade Count:17
Melt Temperature 135 - 338 °C
275 - 640 °F
Average value: 286 °C Grade Count:36
Mold Temperature 35.0 - 121 °C
95.0 - 250 °F
Average value: 95.7 °C Grade Count:53
Drying Temperature 79.0 - 149 °C
174 - 300 °F
Average value: 119 °C Grade Count:35
Moisture Content 0.0200 - 0.0500 %
0.0200 - 0.0500 %
Average value: 0.0211 % Grade Count:28
Dew Point -28.9 °C
-20.0 °F
Average value: -28.9 °C Grade Count:24
Injection Pressure 4.96 - 103 MPa
720 - 15000 psi
Average value: 82.6 MPa Grade Count:42