Arlon Thermabond® 48781A008 0.008" (0.203 mm) Uncured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name Thermabond®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon Thermabond® 48781A008 0.008" (0.203 mm) Uncured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Generation II Thermabond® NP electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner 1: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Uncured Silicone RubberLiner: 2 Polyethylene Product Use: Electrically insulating electronic adhesive. Bonds without primer.Appearance: Blue colored, high viscosity gum.This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 38.1 microns
1.50 mil
Liner 1
38.1 microns
1.50 mil
Liner 2
63.5 microns
2.50 mil
Side 1; Arlon SQA-TMS-003
63.5 microns
2.50 mil
Side 2; Arlon SQA-TMS-003
76.2 microns
3.00 mil
Substrate; Arlon SQA-TMS-003
203 microns
8.00 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Silicone Property; ASTM D2240
Tensile Strength 5.17 MPa
750 psi
Silicone Property; ASTM D412
Elongation at Break 400 %
400 %
Silicone Property; ASTM D412
Poissons Ratio 0.50
0.50
Approximately, Silicone Property
Shear Modulus 0.000207 GPa
0.0300 ksi
ASTM 1002
Shear Strength 2.76 MPa
400 psi
Lap; ASTM 1002
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
11.1 µin/in-°F
ASTM E 831
CTE, linear, Transverse to Flow 20.0 µm/m-°C
11.1 µin/in-°F
ASTM E 831
Specific Heat Capacity 0.980 J/g-°C
0.234 BTU/lb-°F
Silicone Property; E1461-01
Thermal Conductivity 0.300 W/m-K
2.08 BTU-in/hr-ft²-°F
Product Property; ASTM E 1530
0.400 W/m-K
2.78 BTU-in/hr-ft²-°F
Silicone Property; ASTM E 1530
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -73.3 °C
-100 °F
Glass Transition Temp, Tg <= -100 °C
<= -148 °F
Silicone Property; ASTM D3418
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 3.3

@Frequency 1.00e+6 Hz
3.3

@Frequency 1.00e+6 Hz
Silicon Property; IPC TM 650 - 2.5.5.3
3.5

@Frequency 1.00e+6 Hz
3.5

@Frequency 1.00e+6 Hz
Product Property; IPC TM 650 - 2.5.5.3
Dielectric Strength 39.0 kV/mm
990 kV/in
ASTM D149
Dissipation Factor 0.0045

@Frequency 1.00e+6 Hz
0.0045

@Frequency 1.00e+6 Hz
Silicon Property; IPC TM 650 - 2.5.5.3
0.0045

@Frequency 1.00e+6 Hz
0.0045

@Frequency 1.00e+6 Hz
Product Property; IPC TM 650 - 2.5.5.3
Processing Properties Metric English Comments
Cure Time 15.0 min

@Pressure 0.0689 - 0.345 MPa,
Temperature 121 °C
0.250 hour

@Pressure 10.0 - 50.0 psi,
Temperature 250 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 4.44 - 10.0 °C
6.00 Month

@Temperature 40.0 - 50.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Blue
Total Product Weight (g/m2) 240
Arlon SQA-TMS-025