Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Murtfeldt Muralen® plus + AB Polyethylene, Antibacterial Muralen® is based on high molecular weight polyethylene (PE-HMW) and is ideally suited for use in applications that require the generally impressive material properties of polyethylene. Because of.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Nylacast Aquanyl Nylon 612 Copolymer Aquanyl is a copolymer of Nylon 6 and Nylon 12 produced via the anionic polymerization process using the monomer's Caprolactam and Laurinlactam. It has reduced water absorption, improved stability a.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Nylacast Cast Nylon 6, Glass Filled Information provided by Nylacast Ltd. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Nylacast H.S. Blue Cast Nylon 6, Heat Stabilized HS Blue is a heat Stabilised Cast Nylon 6. Its mechanical properties are maintained when operating at higher temperature and improves mechanical properties. This helps to reduce the stress distortio.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Nylacast Nylube Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant) This supreme wear resistant grade contains a combined liquid/solid lubricant system, which allows for a coefficient of friction as low as 0.08. The material has outstanding Pressure-Velocity capabil.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Nylacast Nylube GF Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant), Glass Filled For applications requiring higher compressive strength the NYLUBE GF masterbatch incorporates hollow glass ovule, designed to float and evenly distribute through the polymerising polymer. The glass .. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Polikim ULPOLEN® 500 UHMWPE Standard Standard Ulpolen® 1000 is the universal type primarily preferred on the condition that its technical properties meet operating environment requirements. It is more cost efficient compared to specia.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Quadrant EPP Cesticolor™ HD 500 Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Quadrant EPP Cestilene™ HD 500 Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Minimum Service Temperature, Air | -100 - -40.0 °C | -148 - -40.0 °F | Average value: -55.0 °C Grade Count:3 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Global EPP PA 6C Cast Polyamide 6 Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Global EPP PA 6C OFN Cast Polyamide 6 + Blended Liquid Lubricant Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Global EPP PA 6C WFN Cast Polyamide 6 + Wax Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Lord Adhesives Circalokâ„¢ 6031 A/B Epoxy Encapsulant Circalokâ„¢ 6031 A/B is a two-part epoxy potting compound with excellent electrical properties at elevated temperatures. Good arc-track resistance under high voltage loading and other dielectric .. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Continuous; DIN 52612 |
Isoflon PEHD 500 High Density Polyethylene Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Continuous |
Schwartz Technical Plastics LAMIGAMID® 700 Ultra High Molecular Weight Polyethylene Application: wear liners, sliding platesInformation provided by Schwartz Technical Plastics GmbH |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Shin-Etsu Silicones KE-5006BU Low Temperature Silicone Elastomer ShinEtsu KE5006B U is a phenyl (PVMQ) silicone compound. This product is designed for good low temperature characteristics.Product Features: A broad range of service temperatures from 100 to +260°.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Shin-Etsu Silicones KE-5006U PVMQ Silicone ShinEtsu KE5006 U is a phenyl (PVMQ) silicone product. This product is designed for good low temperature characteristics.Product Features:A broad range of service temperatures from 100 to +260°C .. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Shin-Etsu Silicones X-30-1028U Low Temperature Silicone Elastomer ShinEtsu X301028U is a phenyl (PVMQ) silicone base. This product is designed for good low temperature characteristics. Product Features: A broad range of service temperatures from 100 to +260°C (.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Zeus ETFE Tubing ETFE (Ethylenetetrafluoroethylene), a copolymer of ethylene and tetrafluoroethylene, is used in applications requiring excellent impact, abrasion and stress cracking resistance. This polymer possess.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | DSC |
Adamas Adalon® 203 PTFE, 15/5% Glass/Graphite Filled Information provided by Adamas, HPM |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | DSC |
Adamas Adalon® 812 PTFE, 46% Bronze, Green Information provided by Adamas, HPM |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Arlon CP-594CX Bulk Compound Product Use: Electrically insulating electronic adhesive. Bonds without primer.Appearance: Gray, high viscosity gumUL94V-0: The product is designed to meet UL94V-0 flame resistance requirements but .. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Arlon Thermabond® 99A30N008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Arlon Thermabond® 99A50X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Arlon Thermabond® 99A90X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Arlon Thermabond® R37260N008 0.008" Uncured Silicone Rubber on Fiberglass Carrier Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction:Liner: 1 mil FEPProduct: Uncured Silicone RubberCarrier: 3 m.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Arlon Thermabond® R37300X008 0.008" Uncured Silicone Rubber on Fiberglass Carrier Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction:Liner: 1 mil FEPProduct: Uncured Silicone RubberCarrier: 3 m.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | DSC |
Adamas Adalon® 463 PTFE, 15% Special Polyimide Information provided by Adamas, HPM |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Continuous |
Isoflon ETFE Fluoropolymer material specifications.Information provided by Isoflon. |