Material Notes:
ETFE (Ethylenetetrafluoroethylene), a copolymer of ethylene and tetrafluoroethylene, is used in applications requiring excellent impact, abrasion and stress cracking resistance. This polymer possesses superior toughness, stiffness and durability, all while being chemically inert. The material can be extruded in variety of forms, including flexible convoluted tubing that meets Mil Spec 81914 certification.
Physical Properties Metric English Comments
Density 1.70 - 1.86 g/cc
0.0614 - 0.0672 lb/in³
ASTM D792
Water Absorption 0.0070 %
0.0070 %
ASTM D257
Crystallinity 50 %
50 %
Mechanical Properties Metric English Comments
Hardness, Shore D 63 - 72
63 - 72
ASTM D2240
Tensile Strength, Ultimate 37.0 - 50.0 MPa
5370 - 7250 psi
ASTM D638
Elongation at Break 200 - 550 %
200 - 550 %
ASTM D638
Modulus of Elasticity 0.490 - 0.780 GPa
71.1 - 113 ksi
ASTM D638
Flexural Modulus 0.700 - 1.20 GPa
102 - 174 ksi
ASTM D790
Coefficient of Friction 0.050 - 0.40
0.050 - 0.40
Thermal Properties Metric English Comments
CTE, linear 50.0 - 90.0 µm/m-°C

@Temperature 20.0 °C
27.8 - 50.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 230 - 282 °C
446 - 540 °F
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -100 °C
-148 °F
Glass Transition Temp, Tg 40.0 - 80.0 °C
104 - 176 °F
Decomposition Temperature 350 - 380 °C
662 - 716 °F
ASTM E1131
Oxygen Index 30 - 46 %
30 - 46 %
ASTM D2863
Optical Properties Metric English Comments
Refractive Index 1.34
1.34
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
ASTM D257
Dielectric Constant 2.5 - 2.6

@Frequency 1.00e+6 Hz
2.5 - 2.6

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 15.7 - 70.9 kV/mm
400 - 1800 kV/in
ASTM D149
Descriptive Properties Value Comments
Radiation Resistance (MRad) 50