Nylacast H.S. Blue Cast Nylon 6, Heat Stabilized

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Heat Stabilized
Manufacturer Nylacast
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylacast H.S. Blue Cast Nylon 6, Heat Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HS Blue is a heat Stabilised Cast Nylon 6. Its mechanical properties are maintained when operating at higher temperature and improves mechanical properties. This helps to reduce the stress distortion that can be caused by machining.Information provided by Nylacast Ltd.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
method A; ISO 1183:1987
Mechanical Properties Metric English Comments
Hardness, Shore D 83 - 85
83 - 85
ISO 868:2003
Tensile Strength, Yield 80.0 MPa
11600 psi
Type 1B, 50mm/min; ISO 527-1/2:1993
Elongation at Break >= 20 %
>= 20 %
Type 1B, 50mm/min; ISO 527-1/2:1993
Tensile Modulus 3.487 GPa
505.7 ksi
Type 1B, 50mm/min; ISO 527-1/2:1993
Flexural Strength 100 - 114 MPa
14500 - 16500 psi
1.5mm/min; ISO 178:2001
Flexural Modulus 2.90 GPa
421 ksi
1.5mm/min; ISO 178:2001
Compressive Strength 90.0 - 147 MPa
13100 - 21300 psi
Type B, 5mm/min; ISO 604:2002
Compressive Modulus 2.70 GPa
392 ksi
Type B, 5mm/min; ISO 604:2002
Izod Impact, Notched (ISO) 5.40 kJ/m²
2.57 ft-lb/in²
Type A; ISO 180:2000
Coefficient of Friction, Dynamic 0.15

@Pressure 1.75 MPa
0.15

@Pressure 254 psi
31.4m/min
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
44.4 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2:1999
Melting Point 223.6 °C
434.5 °F
Maximum Service Temperature, Air 180 °C
356 °F
Intermittent
115 °C

@Time 1.80e+7 sec
239 °F

@Time 5000 hour
Continuous
Minimum Service Temperature, Air -100 °C
-148 °F
Intermittent
-40.0 °C
-40.0 °F
Continuous
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093:1980-01
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093:1980-01
Dielectric Constant 3.7

@Frequency 1.00e+6 Hz
3.7

@Frequency 1.00e+6 Hz
IEC 60250:1969-01
4.0

@Frequency 100 Hz
4.0

@Frequency 100 Hz
IEC 60250:1969-01
Dielectric Strength 25.0 kV/mm
635 kV/in
IEC 60243-1:1998-01
Comparative Tracking Index 600 V
600 V
IEC 60112:2003-01
Descriptive Properties Value Comments
Color Blue