Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Murtfeldt Material ”S”® 1000 RB Polyethylene, High Friction An elastomer in Material ”S”® 1000 RB gives it high impact resistance and skid resistance.Special Properties:• High coefficient of friction• Good wear and abrasion resistanceInformation provide.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Murtfeldt Muralen® Polyethylene Muralen® is based on high molecular weight polyethylene (PE-HMW) and is ideally suited for use in applications that require the generally impressive material properties of polyethylene. Because of.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Nylacast Aquanyl Nylon 612 Copolymer Aquanyl is a copolymer of Nylon 6 and Nylon 12 produced via the anionic polymerization process using the monomer's Caprolactam and Laurinlactam. It has reduced water absorption, improved stability a.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Nylacast Nylube MO Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant), MoS2 Filled The combined Nylube lubrication system incorporating fine particles of molybdenum disulphide provides enhanced load bearing capabilities while retaining Nylube's excellent frictional characteristics.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Nylacast Oilon Cast Nylon 6, Lubricated (Lubricant Oil Filled) This exceptional oil-loaded nylon features a complex blended oil lubrication system, uniformly distributed throughout the product, that guarantees constant performance over the whole service life. E.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Polikim ULPOLEN® 500 UHMWPE Standard Standard Ulpolen® 1000 is the universal type primarily preferred on the condition that its technical properties meet operating environment requirements. It is more cost efficient compared to specia.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
GEHR Plastics PSU Polysulfone Polysulfone shows great thermal stability. It possesses a high mechanical strength, very good dielectric properties and hydrolysis resistance and a high radiation resistance. PSU has a low notch imp.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Global EPP PA 6C HS BLUE Cast Polyamide 6 + UV and Heat Stabilizers Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Global EPP PA 6C IMPACT Cast Polyamide 6 + Plasticizer Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Global EPP PA 6C OFN Cast Polyamide 6 + Blended Liquid Lubricant Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Lord Adhesives Circalokâ„¢ 6031 A/B Epoxy Encapsulant Circalokâ„¢ 6031 A/B is a two-part epoxy potting compound with excellent electrical properties at elevated temperatures. Good arc-track resistance under high voltage loading and other dielectric .. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Global EPP PA 612 Copolymer Cast Polyamide 612 Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Shin-Etsu Silicones KE-5006BU Low Temperature Silicone Elastomer ShinEtsu KE5006B U is a phenyl (PVMQ) silicone compound. This product is designed for good low temperature characteristics.Product Features: A broad range of service temperatures from 100 to +260°.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Shin-Etsu Silicones KE-5006U PVMQ Silicone ShinEtsu KE5006 U is a phenyl (PVMQ) silicone product. This product is designed for good low temperature characteristics.Product Features:A broad range of service temperatures from 100 to +260°C .. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Shin-Etsu Silicones X-30-1028U Low Temperature Silicone Elastomer ShinEtsu X301028U is a phenyl (PVMQ) silicone base. This product is designed for good low temperature characteristics. Product Features: A broad range of service temperatures from 100 to +260°C (.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Continuous |
Wolf Kunststoff ZEDEX® ZX-100A Polymer Alloy Main Characteristics: Tough; Resilient; Soft; Low cost solutionApplications: Handling, Vessel and pump, Steel and Water, Chemical Engineering, Automitve Technology, Machine ToolsInformation provided.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | DSC |
Adamas Adalon® 814 PTFE, 55% Bronze, 5% MoS2 Information provided by Adamas, HPM |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | DSC |
Adamas Adalon® 817 PTFE, 60% Bronze Information provided by Adamas, HPM |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Arlon Thermabond® 99A50X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Arlon Thermabond® 99A60X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Arlon Thermabond® R37623X008 0.0050" Cured Silicone Rubber with Fiberglass Substrate Thermabond®: Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction:Side 1: Cured Silicone RubberSubstrate: 1080-style FiberglassSide 2: Cured Silico.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | DSC |
Adamas Adalon® 463 PTFE, 15% Special Polyimide Information provided by Adamas, HPM |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | DSC |
Adamas Adalon® 816 PTFE, 46% Bronze, Blue Information provided by Adamas, HPM |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | DSC |
Adamas Rixon U PEEK, Unreinforced Information provided by Adamas, HPM |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Continuous |
Isoflon ETFE Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Minimum Service Temperature, Air | -100 - -20.0 °C | -148 - -4.00 °F | Average value: -45.1 °C Grade Count:34 |
Overview of materials for Nylon 6, Cast This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Minimum Service Temperature, Air | -100 - -40.0 °C | -148 - -40.0 °F | Average value: -52.9 °C Grade Count:11 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |