Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shin-Etsu Silicones X-30-1028U Low Temperature Silicone Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Shin-Etsu Silicones
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones X-30-1028U Low Temperature Silicone Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ShinEtsu X301028U is a phenyl (PVMQ) silicone base. This product is designed for good low temperature characteristics. Product Features: A broad range of service temperatures from 100 to +260°C (148 to +500°F.)Typical Applications: Low temperature gaskets.Low temperature packing.Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 31
31
Tensile Strength at Break 10.78 MPa
1564 psi
Elongation at Break 930 %
930 %
Tear Strength 28.4 kN/m
162 pli
Die B
Compression Set 35 %

@Temperature 150 °C,
Time 79200 sec
35 %

@Temperature 302 °F,
Time 22.0 hour
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -100 °C
-148 °F
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 200 °C
4.00 hour

@Temperature 392 °F
Post
Descriptive Properties Value Comments
Cure Agent DBPH-50
Cure Type Post Cure
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved