Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon Thermabond® R37260N008 0.008" Uncured Silicone Rubber on Fiberglass Carrier

Category Polymer , Thermoset , Silicone , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name Thermabond®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon Thermabond® R37260N008 0.008" Uncured Silicone Rubber on Fiberglass Carrier.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction:Liner: 1 mil FEPProduct: Uncured Silicone RubberCarrier: 3 mil PTFE coated fiberglassThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 2.40 g/cc
0.0867 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 203 microns
8.00 mil
Product; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
Silicone Property; ASTM D2240
Tensile Strength 2.76 MPa
400 psi
Silicone Property; ASTM D412
Tensile Strength, Yield 3.45 MPa

@Strain <=1.00 %
500 psi

@Strain <=1.00 %
Silicone Property; Arlon SQA-TMS-008
Elongation at Break 245 %
245 %
Silicone Property; ASTM D412
Poissons Ratio 0.50
0.50
Shear Modulus 1.03 GPa
149 ksi
Product Property; ASTM D1002
Shear Strength 2.00 MPa
290 psi
Lap; Product Property; ASTM D1002
Thermal Properties Metric English Comments
CTE, linear 134 µm/m-°C
74.4 µin/in-°F
Silicone Property; ASTM E831
Specific Heat Capacity 0.920 J/g-°C

@Temperature 100 °C
0.220 BTU/lb-°F

@Temperature 212 °F
Silicone Property; ASTM E1952
Thermal Conductivity 1.00 W/m-K

@Temperature 100 °C
6.94 BTU-in/hr-ft²-°F

@Temperature 212 °F
Silicone Property; ASTM E1530
Maximum Service Temperature, Inert 204 °C
399 °F
Minimum Service Temperature, Air -100 °C
-148 °F
Glass Transition Temp, Tg -118 °C
-180 °F
Silicone Property; ASTM D3418
Electrical Properties Metric English Comments
Dielectric Constant 5.4

@Frequency 1.00e+6 Hz
5.4

@Frequency 1.00e+6 Hz
Silicone Property; IPC TM 650 - 2.5.5.3
Dielectric Strength 30.9 kV/mm
785 kV/in
ASTM D149
Dissipation Factor 0.0050

@Frequency 1.00e+6 Hz
0.0050

@Frequency 1.00e+6 Hz
Silicone Property; IPC TM 650 - 2.5.5.3
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 121 °C
0.250 hour

@Temperature 250 °F
Recommended Cure Cycle; After Thermabond® reaches temperature
Shelf Life 6.00 Month

@Temperature 7.22 °C
6.00 Month

@Temperature 45.0 °F
Descriptive Properties Value Comments
Color Gray
Plasticity (mm) 2
Arlon SQA-TMS-005
Thermal Resistance (°C-in2/W) 0.32
ASTM E1530
Total Product Weight (oz/yd2) 14.3
Arlon SQA-TMS-025