Nylacast Nylube GF Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant), Glass Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Fiber/Solid Lube Filled
Manufacturer Nylacast
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylacast Nylube GF Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant), Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For applications requiring higher compressive strength the NYLUBE GF masterbatch incorporates hollow glass ovule, designed to float and evenly distribute through the polymerising polymer. The glass additive allows the material to operate at higher maximum service temperatures while the wax counteracts the deteriorating surface slip characteristics making this product an outstanding abrasion and temperature resistant material at high loads.Information provided by Nylacast Ltd.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
method A; ISO 1183:1987
Mechanical Properties Metric English Comments
Tensile Strength, Yield 70.0 MPa
10200 psi
Type 1B, 50mm/min; ISO 527-1/2:1993
Elongation at Break >= 10 %
>= 10 %
Type 1B, 50mm/min; ISO 527-1/2:1993
Tensile Modulus 3.00 GPa
435 ksi
Type 1B, 50mm/min; ISO 527-1/2:1993
Flexural Strength 115 MPa
16700 psi
1.5mm/min; ISO 178:2001
Flexural Modulus 3.00 GPa
435 ksi
1.5mm/min; ISO 178:2001
Compressive Strength 105 MPa
15200 psi
Type B, 5mm/min; ISO 604:2002
Compressive Modulus 3.00 GPa
435 ksi
Type B, 5mm/min; ISO 604:2002
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
Type A; ISO 180:2000
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
44.4 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2:1999
Melting Point 220 °C
428 °F
Maximum Service Temperature, Air 190 °C
374 °F
Intermittent
120 °C

@Time 1.80e+7 sec
248 °F

@Time 5000 hour
Continuous
Minimum Service Temperature, Air -100 °C
-148 °F
Intermittent
-40.0 °C
-40.0 °F
Continuous
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093:1980-01
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093:1980-01
Dielectric Constant 3.7

@Frequency 1.00e+6 Hz
3.7

@Frequency 1.00e+6 Hz
IEC 60250:1969-01
4.0

@Frequency 100 Hz
4.0

@Frequency 100 Hz
IEC 60250:1969-01
Dielectric Strength 25.0 kV/mm
635 kV/in
IEC 60243-1:1998-01
Comparative Tracking Index 600 V
600 V
IEC 60112:2003-01
Descriptive Properties Value Comments
Color Black