Tensile Strength, Ultimate 55.2 - 103 MPa
8000 - 15000 psi
Average value: 74.7 MPa Grade Count:6
Overview of materials for PPE/PPO + Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "PPE/PPO + Carbon Fiber". Each property range of values reported is minimum and maximum values of appropr..
Tensile Strength, Ultimate 53.8 - 103 MPa
7800 - 15000 psi
Average value: 83.6 MPa Grade Count:25
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe..
Tensile Strength, Ultimate 48.3 - 103 MPa
7000 - 15000 psi
Average value: 79.0 MPa Grade Count:10
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Tensile Strength, Ultimate 23.0 - 103 MPa
3340 - 15000 psi
Average value: 49.2 MPa Grade Count:36
Overview of materials for Acetal Copolymer, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu..
Tensile Strength, Ultimate 50.0 - 103 MPa
7250 - 15000 psi
Average value: 69.7 MPa Grade Count:7
Overview of materials for Polybutylene Terephthalate (PBT), Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Aramid Fiber Filled". Each property range of values reported is minimu..